Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® Resist zk5BR - PMMA-I - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® Resist zk5BR:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Productprofil:

PLEXIGLAS® Resist zk5BR is an amorphous, impact-modified thermoplastic molding compound (PMMA-I).

 

Typical properties of impact-modified PLEXIGLAS® molding compounds are:

 

  • high weather resistance
  • excellent transmission and clarity
  • brilliant appearance
  • the pleasant feel and sound of the moldings.

 

PLEXIGLAS® Resist zk5BR is characterized by the following special properties:

 

  • high break resistance and impact strength
  • improved resistance to stress cracking
  • balanced property profile
  • AMECA listing.

Application:

Used for injection molding as well as for extruding and coextruding panels and profiles

Example:

mobile phone displays, extruded and injection-molded luminaire covers, extruded hollow profiles, writing utensils such as stencils and fountain pens, housings, coextruded profiles for window frames, gutters, downspouts, and housewares such as cutlery handles, bowls, cookie jars.

Processing:

PLEXIGLAS® Resist zk5BR molding compound can be processed on machines with 3-zone general purpose screws for engineering thermoplastics.

Physical Form / Packaging:

PLEXIGLAS® Resist zk molding compounds are supplied as pellets of uniform size in 25kg polyethylene bags or in 500kg boxes with PE lining; other packaging on request.

加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 3.3 cm³/10min ISO 1133
温度 230 °C -
载荷 3.8 kg -
熔体密度 1040 kg/m³ -
熔体 0.19 W/(m K) -
熔体的比热 2440 J/(kg K) -
有效导热率a 7.49E-8 m²/s -
喷射温度 80 °C -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2400 MPa ISO 527
屈服应力 62 MPa ISO 527
屈服伸长率 4.5 % ISO 527
名义断裂伸长率 27 % ISO 527
拉伸蠕变模量, 1h 2000 MPa ISO 899-1
拉伸蠕变模量, 1000h 1500 MPa ISO 899-1
无缺口简支梁冲击强度, +23°C 50 kJ/m² ISO 179/1eU
热性能价值单位Test Standard
ISO数据
玻璃化转变温度, 10°C/min 109 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 93 °C ISO 75-1/-2
热变形温度, 0.45 MPa 98 °C ISO 75-1/-2
维卡软化温度, B 100 °C ISO 306
线性热膨胀系数, 平行 90 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.6 mm -
Yellow Card 现存 是的 - -
燃烧速率, FMVSS, 厚度:1毫米 89.3 mm/min ISO 3795 (FMVSS 302)
燃烧性-氧指数 17.5 % ISO 4589-1/-2
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 3.7 - IEC 62631-2-1
相对介电常数., 1MHz 2.9 - IEC 62631-2-1
介质损耗因子, 100Hz 500 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 300 E-4 IEC 62631-2-1
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
表面电阻率 1E13 Ohm IEC 62631-3-2
相对漏电起痕指数 600 - IEC 60112
光学特性价值单位Test Standard
ISO Data
光输送 92 % ISO 13468-1, -2
其它性能价值单位Test Standard
吸水性 2 % 类似ISO 62
吸湿性 0.6 % 类似ISO 62
密度 1170 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 250 °C ISO 294
注塑, 模具温度 62 °C ISO 294
注塑, 注射速度 195 mm/s ISO 294
加工推荐(注塑)价值单位Test Standard
预干燥-温度 90 °C -
预干燥-时间 2 - 3 h -
注塑熔体温度 220 - 260 °C -
模具温度 50 - 70 °C -
函数
粘度-剪切速度 , PLEXIGLAS® Resist zk5BR, PMMA-I, Röhm
剪切应力-剪切速度 , PLEXIGLAS® Resist zk5BR, PMMA-I, Röhm
动态剪切模量-温度 , PLEXIGLAS® Resist zk5BR, PMMA-I, Röhm
应力-应变.  , PLEXIGLAS® Resist zk5BR, PMMA-I, Röhm
正割模量-应变.  , PLEXIGLAS® Resist zk5BR, PMMA-I, Röhm
应力-应变(等时的) 23°C, PLEXIGLAS® Resist zk5BR, PMMA-I, Röhm
蠕变模量-时间. 23°C, PLEXIGLAS® Resist zk5BR, PMMA-I, Röhm
蠕变曲线 23°C, PLEXIGLAS® Resist zk5BR, PMMA-I, Röhm
单位质量比焓-温度(DSC) , PLEXIGLAS® Resist zk5BR, PMMA-I, Röhm
拉伸模量-温度 , PLEXIGLAS® Resist zk5BR, PMMA-I, Röhm
典型数据
加工方法
注塑, 薄膜挤出成型, 异型材挤出成型, 片材挤出成型, 其它挤出成型, 热成型
供货形式
粒料
添加剂
脱模助剂
特殊性能
高冲击韧性的/经抗冲改性的, 经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 透明.
特征
无定形
耐化学试剂
耐环境应力裂纹性
应用
建材, 封装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
PREPROCESSING
Predrying temperature: max. 90 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 220 - 260°C
Mold temperature:50 - 70°C
E尾募烦龀尚
PREPROCESSING
Predrying temperature: max. 90 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 220 - 260 °C
Die temperature: 220 - 260 °C
板材挤出成型
PREPROCESSING
Predrying temperature: max. 90 °C
Predrying time in a desiccant-type drier: 2 - 3 h
PROCESSING
Melt temperature: 220 - 260 °C
Die temperature: 220 - 260 °C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.