Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TPE ProvaMed® 1060 - TPE - ACTEGA DS GmbH

Material Data Center offers the following functions for TPE ProvaMed® 1060:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, CAE Interfaces

Check here, which other Provamed datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 8 g/10min ISO 1133
温度 230 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
100%应变时的应力 1.7 MPa ISO 527
断裂应变. TPE >300 % ISO 527
23°C时恒定应变下的永久变形, 24h 18 % ISO 815
70°C时恒定应变下的永久变形, 24h 91 % ISO 815
ASTM数据
邵氏硬度A 60 - ASTM D 2240
邵氏硬度D 15 - ASTM D 2240
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 162 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min -40 °C ISO 11357-1/-2
其它性能价值单位Test Standard
密度 890 kg/m³ ISO 1183
加工推荐(注塑)价值单位Test Standard
模具温度 20 - 60 °C -
加料温度 20 - 30 °C -
1区 140 - 230 °C -
喷嘴温度 190 - 230 °C -
典型数据
加工方法
注塑, 其它挤出成型
供货形式
粒料
特殊性能
透明., 消毒, 环氧乙烷灭菌(EtO), 蒸汽灭菌, Gamma irradiation sterilization
耐化学试剂
抗氧化性, 抗辐射性
Certifications
医用级, Biocompatibility ISO 10993
应用
药物
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.