Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AESNO P201 TL - PA12-I - ARKEMA

Material Data Center offers the following functions for Rilsamid® AESNO P201 TL:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Rilsamid® AESNO P201 TL resin is a natural polyamide 12. This grade is plasticized and designed for tube extrusion.

Rilsamid® AESNO P201 TL resin falls into the PA12-PHLY category according to DIN 73378.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 5 / * cm³/10min ISO 1133
温度 235 / * °C -
载荷 5 / * kg -
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 - / 540 MPa ISO 527
屈服应力 - / 27 MPa ISO 527
屈服伸长率 - / 28 % ISO 527
名义断裂伸长率 - / >50 % ISO 527
简支梁缺口冲击强度, -30°C - / 8 kJ/m² ISO 179/1eA
肖氏硬度D 62 / * - ISO 7619-1
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 176 / * °C ISO 11357-1/-3
其它性能干 / 已调节单位Test Standard
密度 1010 / - kg/m³ ISO 1183
函数
应力-应变.  , Rilsamid® AESNO P201 TL (烘干), PA12-I, ARKEMA
正割模量-应变.  , Rilsamid® AESNO P201 TL (烘干), PA12-I, ARKEMA
典型数据
加工方法
异型材挤出成型, 其它挤出成型
供货形式
粒料
添加剂
增塑剂
特殊性能
高冲击韧性的/经抗冲改性的, 经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
地区供应
其他信息
其E烦龀尚
Processing conditions:
- Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 270°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80°C.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.