Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AESNO P302 TL - PA12-I - ARKEMA

Material Data Center offers the following functions for Rilsamid® AESNO P302 TL:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
ISO 16396 - PA12-HIP, EGHL, C22-004

Rilsamid® AESNO P302 TL resin is a natural polyamide. 
This grade is plasticized and designed for tube extrusion.

Rilsamid® AESNO P302 TL resin falls into the PA12-HIPHL category according to DIN 73378.


Main applications:

Air brake. 
Tubing for use in motor vehicles

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf life:
Two years from the date of delivery. for any use above this limit, please refer to our technical services.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 13 / * cm³/10min ISO 1133
温度 235 / * °C -
载荷 5 / * kg -
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 475 / 430 MPa ISO 527
屈服应力 28 / 24 MPa ISO 527
屈服伸长率 24 / 24 % ISO 527
名义断裂伸长率 >50 / >50 % ISO 527
简支梁缺口冲击强度, +23°C 46 / - kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 4 / 6 kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 174 / * °C ISO 11357-1/-3
线性热膨胀系数, 平行 150 / * E-6/K ISO 11359-1/-2
电性能干 / 已调节单位Test Standard
ISO数据
体积电阻率 1E12 / 1E12 Ohm*m IEC 62631-3-1
表面电阻率 * / 7E13 Ohm IEC 62631-3-2
介电强度 41 / 41 kV/mm IEC 60243-1
相对漏电起痕指数 * / 600 - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 1.2 / * % 类似ISO 62
密度 1030 / 1030 kg/m³ ISO 1183
函数
粘度-剪切速度 , Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
剪切应力-剪切速度 , Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
动态剪切模量-温度 , Rilsamid® AESNO P302 TL (烘干), PA12-I, ARKEMA
应力-应变.  , Rilsamid® AESNO P302 TL (烘干), PA12-I, ARKEMA
正割模量-应变.  , Rilsamid® AESNO P302 TL (烘干), PA12-I, ARKEMA
应力-应变(等时的) 23°C, Rilsamid® AESNO P302 TL (烘干), PA12-I, ARKEMA
蠕变模量-时间. 23°C, Rilsamid® AESNO P302 TL (烘干), PA12-I, ARKEMA
蠕变曲线 23°C, Rilsamid® AESNO P302 TL (烘干), PA12-I, ARKEMA
LTHA-断裂伸长率 2mm, Rilsamid® AESNO P302 TL, PA12-I, ARKEMA
典型数据
加工方法
注塑, 异型材挤出成型, 其它挤出成型
供货形式
粒料
添加剂
润滑剂, 增塑剂
特殊性能
高冲击韧性的/经抗冲改性的, 经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
地区供应
其他信息
E尾募烦龀尚

Processing conditions, Extrusion :

- Typical melt temperature (Min / Recommended / Max) : 200°C / 220°C / 240°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80°C.

权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.