Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AMNO P40 TLD - PA12 - ARKEMA

Material Data Center offers the following functions for Rilsamid® AMNO P40 TLD:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
PA12-P, MHLR, 12-004
Rilsamid® AMNO P40 TLD resin is a natural polyamide. This grade is plasticized and designed for injection molding.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 51 / * cm³/10min ISO 1133
温度 235 / * °C -
载荷 2.16 / * kg -
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 440 / 420 MPa ISO 527
屈服应力 26 / 24 MPa ISO 527
屈服伸长率 26 / 26 % ISO 527
名义断裂伸长率 >50 / >50 % ISO 527
简支梁缺口冲击强度, +23°C - / 25 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C - / 4 kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 171 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 46 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 125 / * °C ISO 75-1/-2
维卡软化温度, B 132 / * °C ISO 306
线性热膨胀系数, 平行 140 / * E-6/K ISO 11359-1/-2
电性能干 / 已调节单位Test Standard
ISO数据
相对介电常数., 100Hz 12 / - - IEC 62631-2-1
相对介电常数., 1MHz 4 / - - IEC 62631-2-1
介质损耗因子, 100Hz 2550 / - E-4 IEC 62631-2-1
介质损耗因子, 1MHz 1290 / - E-4 IEC 62631-2-1
体积电阻率 - / 1E9 Ohm*m IEC 62631-3-1
表面电阻率 * / 5E11 Ohm IEC 62631-3-2
介电强度 - / 24 kV/mm IEC 60243-1
相对漏电起痕指数 * / 600 - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 1.2 / * % 类似ISO 62
密度 1040 / 1040 kg/m³ ISO 1183
函数
粘度-剪切速度 , Rilsamid® AMNO P40 TLD, PA12, ARKEMA
剪切应力-剪切速度 , Rilsamid® AMNO P40 TLD, PA12, ARKEMA
应力-应变(等时的) 23°C, Rilsamid® AMNO P40 TLD (烘干), PA12, ARKEMA
蠕变模量-时间. 23°C, Rilsamid® AMNO P40 TLD (烘干), PA12, ARKEMA
蠕变曲线 23°C, Rilsamid® AMNO P40 TLD (烘干), PA12, ARKEMA
典型数据
加工方法
注塑
供货形式
粒料
添加剂
脱模助剂, 增塑剂
特殊性能
经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
地区供应
其他信息
注塑成型

Processing conditions, Injection:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 270°C.
- Mold temperature : 20 - 40°C
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80 - 90°C.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.