Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® BECNO TL - PA11 - ARKEMA

Material Data Center offers the following functions for Rilsan® BECNO TL:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
PA11, KHL, 12-010
Rilsan® BECNO TL resin is a polyamide produced from a renewable source. This natural grade is designed for cable coating. 11



Main applications:
  • Wire and cable sheathing


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 30 / * cm³/10min ISO 1133
温度 235 / * °C -
载荷 2.16 / * kg -
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 1470 / 1330 MPa ISO 527
屈服应力 43 / 42 MPa ISO 527
屈服伸长率 5 / 5 % ISO 527
名义断裂伸长率 >50 / >50 % ISO 527
简支梁缺口冲击强度, +23°C - / 9 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C - / 10 kJ/m² ISO 179/1eA
冲孔最大力, -30°C - / 5500 N ISO 6603-2
冲孔功, -30°C - / 65 J ISO 6603-2
肖氏硬度D 70 / * - ISO 7619-1
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 189 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 55 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 150 / * °C ISO 75-1/-2
维卡软化温度, B 160 / * °C ISO 306
线性热膨胀系数, 平行 90 / * E-6/K ISO 11359-1/-2
电性能干 / 已调节单位Test Standard
ISO数据
相对介电常数., 100Hz 3 / - - IEC 62631-2-1
相对介电常数., 1MHz 3 / - - IEC 62631-2-1
介质损耗因子, 100Hz 274 / - E-4 IEC 62631-2-1
介质损耗因子, 1MHz 166 / - E-4 IEC 62631-2-1
体积电阻率 - / 1E12 Ohm*m IEC 62631-3-1
表面电阻率 * / 1E14 Ohm IEC 62631-3-2
介电强度 - / 30 kV/mm IEC 60243-1
相对漏电起痕指数 * / 600 - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 1.9 / * % 类似ISO 62
密度 1030 / 1030 kg/m³ ISO 1183
Biobased content 98 % -
函数
粘度-剪切速度 , Rilsan® BECNO TL, PA11, ARKEMA
剪切应力-剪切速度 , Rilsan® BECNO TL, PA11, ARKEMA
应力-应变.  , Rilsan® BECNO TL (烘干), PA11, ARKEMA
正割模量-应变.  , Rilsan® BECNO TL (烘干), PA11, ARKEMA
典型数据
加工方法
注塑, 其它挤出成型
供货形式
粒料
添加剂
润滑剂
特殊性能
经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
Certifications
生物相容
地区供应
其他信息
其E烦龀尚

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 240°C / 250°C / 260°C.

- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80-90°C.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.