Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® BESHV BLK T - PA11 - ARKEMA

Material Data Center offers the following functions for Rilsan® BESHV BLK T:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Ri​lsan® BESHV BLK T is an ultra high viscosity Polyamide 11 grade specifically designed to be extruded into large diameter thick wall pipe. This grade has been specifically engineered to achieve an outstanding balance of properties for Oil & Gas piping applications. It offers a cost effective system for non-metallic corrosion free fluid transfer in critical Oil and Gas industry applications. Rilsan® Polyamide 11 is a thermoplastic material permitted by the US Department of Transportation (DOT) under the Code of Federal Regulations (CFR) Title 49, Part 192, for gas distribution piping to be installed and operated at pressures up to and including 250 psi in a design factor of 0.40.




Main applications:
  • Oil and Gas piping applications


Packaging:

This grade is delivered dried in sealed packaging ready to be processed. For best results in gas pipe extrusion, additional desiccant bed drying to maintain/achieve moisture values <0.02% is recommended.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 - / 1390 MPa ISO 527
屈服应力 - / 42 MPa ISO 527
屈服伸长率 - / 5 % ISO 527
名义断裂伸长率 - / >50 % ISO 527
简支梁缺口冲击强度, +23°C - / 10 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C - / 11 kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 189 / * °C ISO 11357-1/-3
其它性能干 / 已调节单位Test Standard
密度 1030 / - kg/m³ ISO 1183
Biobased content 95 % -
典型数据
加工方法
注塑, 管材挤出, 异型材挤出成型
供货形式
粒料, 黑色
Certifications
生物相容
地区供应
其他信息
注塑成型

PROCESSING CONDITIONS*

Melt Temperature: (Min / Recommended / Max) 240°C / 270°C / 290°C.

Mold: (Temperature) 20-60°C.

Drying: (Time / Temperature / Desiccant Bed Dryer) 12 hours / 80°C / -40°C.

*only necessary for bags opened for more than two hours
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.