Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® BZM 30 O TL - PA11-GF30 - ARKEMA

Material Data Center offers the following functions for Rilsan® BZM 30 O TL:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
PA11, MHLR, 18-070, GF30

Rilsan® BZM 30 O TL is a fiberglass reinforced polyamide 11 produced from a renewable source. This natural grade is designed for injection molding.

According to ASTM D6866, the biobased carbon content is measured at 100%.





Main applications:
  • Quick connectors

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 9 / * cm³/10min ISO 1133
温度 235 / * °C -
载荷 5 / * kg -
模塑收缩率, 平行 0.2 / * % ISO 294-4, 2577
模塑收缩率, 垂直 0.8 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 - / 7300 MPa ISO 527
断裂应力 - / 117 MPa ISO 527
断裂伸长率 - / 6 % ISO 527
无缺口简支梁冲击强度, +23°C - / 89 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C - / 96 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C - / 24 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C - / 17 kJ/m² ISO 179/1eA
肖氏硬度D 74 / * - ISO 7619-1
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 189 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 175 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 180 / * °C ISO 75-1/-2
维卡软化温度, B 170 / * °C ISO 306
线性热膨胀系数, 平行 50 / * E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 1.6 / * mm -
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 3.2 / * mm -
燃烧性-氧指数 22 / * % ISO 4589-1/-2
电性能干 / 已调节单位Test Standard
ISO数据
相对介电常数., 100Hz 4 / - - IEC 62631-2-1
相对介电常数., 1MHz 4 / - - IEC 62631-2-1
介质损耗因子, 100Hz 578 / - E-4 IEC 62631-2-1
介质损耗因子, 1MHz 210 / - E-4 IEC 62631-2-1
体积电阻率 - / 7E11 Ohm*m IEC 62631-3-1
表面电阻率 * / 1E14 Ohm IEC 62631-3-2
介电强度 - / 45 kV/mm IEC 60243-1
相对漏电起痕指数 * / 600 - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 1.4 / * % 类似ISO 62
吸湿性 0.5 / * % 类似ISO 62
密度 1250 / 1250 kg/m³ ISO 1183
Biobased content 98 % -
函数
粘度-剪切速度 , Rilsan® BZM 30 O TL, PA11-GF30, ARKEMA
剪切应力-剪切速度 , Rilsan® BZM 30 O TL, PA11-GF30, ARKEMA
应力-应变.  , Rilsan® BZM 30 O TL (烘干), PA11-GF30, ARKEMA
正割模量-应变.  , Rilsan® BZM 30 O TL (烘干), PA11-GF30, ARKEMA
应力-应变(等时的) 23°C, Rilsan® BZM 30 O TL (烘干), PA11-GF30, ARKEMA
蠕变模量-时间. 23°C, Rilsan® BZM 30 O TL (烘干), PA11-GF30, ARKEMA
蠕变曲线 23°C, Rilsan® BZM 30 O TL (烘干), PA11-GF30, ARKEMA
应力-应变(等时的) 80°C, Rilsan® BZM 30 O TL (烘干), PA11-GF30, ARKEMA
蠕变模量-时间. 80°C, Rilsan® BZM 30 O TL (烘干), PA11-GF30, ARKEMA
蠕变曲线 80°C, Rilsan® BZM 30 O TL (烘干), PA11-GF30, ARKEMA
典型数据
加工方法
注塑
供货形式
粒料
添加剂
脱模助剂
特殊性能
经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
Certifications
生物相容
地区供应
其他信息
注塑成型

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 250°C / 270°C / 290°C.
- Mold temperature : 40 - 90°C

- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80-90°C.

权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.