Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SCHULAMID® 6 GF 35 - PA6-GF35 - LyondellBasell Industries

Material Data Center offers the following functions for SCHULAMID® 6 GF 35:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Schulamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
35% glass fibre reinforced PA 6

加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.003 mm/mm ASTM D 955
模压收缩率, TD 0.012 mm/mm ASTM D 955
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 11000 / 7000 MPa ISO 527
断裂应力 180 / 110 MPa ISO 527
断裂伸长率 3.4 / 6 % ISO 527
无缺口简支梁冲击强度, +23°C 90 / N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 70 / - kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 15 / 32 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 10 / - kJ/m² ISO 179/1eA
ASTM数据
断裂伸长率 11 / - % ASTM D 638
热性能干 / 已调节单位Test Standard
ISO数据
热变形温度, 1.80 MPa 210 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 220 / * °C ISO 75-1/-2
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 1.5 / * mm -
Yellow Card 现存 是的 / * - -
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 3.0 / * mm -
Yellow Card 现存 是的 / * - -
ASTM数据
UL94 燃烧性 HB - UL 94
测试厚度 1.5 mm -
DTUL @ 66 psi 215 °C ASTM D 648
DTUL @ 264 psi 210 °C ASTM D 648
电性能干 / 已调节单位Test Standard
ISO数据
体积电阻率 >1E13 / 1E8 Ohm*m IEC 62631-3-1
表面电阻率 * / >1E15 Ohm IEC 62631-3-2
相对漏电起痕指数 450 / - - IEC 60112
其它性能干 / 已调节单位Test Standard
密度 1410 / - kg/m³ ISO 1183
密度 1390 kg/m³ ASTM D 792
模塑测量的特殊性能干 / 已调节单位Test Standard
ISO数据
粘数 145 / * cm³/g ISO 307, 1157, 1628
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 °C -
预干燥-时间 4 - 6 h -
注塑熔体温度 250 - 280 °C -
模具温度 60 - 90 °C -
典型数据
加工方法
注塑
供货形式
碎粒料
添加剂
脱模助剂
地区供应
其他信息
注塑成型
PREPROCESSING; Pretreatment
Predrying: 4-6h / 80°C

PROCESSING ;Processing:

Melttemperature250 - 280°C
Mouldtemperature60 - 90°C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.