Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SCHULAMID® 612 FS 4004 - PA612 - LyondellBasell Industries

Material Data Center offers the following functions for SCHULAMID® 612 FS 4004:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Schulamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
High impact modified Polyamide 612 with very good long term heat stabilization.
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 1100 / 590 MPa ISO 527
屈服应力 35 / 27 MPa ISO 527
屈服伸长率 29 / 36 % ISO 527
无缺口简支梁冲击强度, +23°C N / N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N / - kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 110 / 120 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 70 / - kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
热变形温度, 1.80 MPa 45 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 60 / * °C ISO 75-1/-2
维卡软化温度, B 110 / * °C ISO 306
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 1.5 / * mm -
Yellow Card 现存 是的 / * - -
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 3.0 / * mm -
Yellow Card 现存 是的 / * - -
燃烧速率, FMVSS, 厚度:1毫米 30 mm/min ISO 3795 (FMVSS 302)
其它性能干 / 已调节单位Test Standard
密度 1010 / - kg/m³ ISO 1183
典型数据
加工方法
注塑, 其它挤出成型
特殊性能
高冲击韧性的/经抗冲改性的, 经热稳处理的/耐热的
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.