Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SINKRAL® B4 Milano - ABS - Versalis S.p.A

Material Data Center offers the following functions for SINKRAL® B4 Milano:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Sinkral datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Symbol according to ISO 1043-1: ABS

Designation: Thermoplastics ISO 2580-ABS 1,EGN,105-04-16-20

Sinkral B 4 Milano is a special grade for extrusion/thermoforming.
Thanks to its low gel content toghether an optimum balance of stiffness and impact resistance, ensures high aesthetic quality of surfaces, partcularly suitable for co-extrusion.
Optimal thermal stability and rheological properties also permit the sheet production of large dimensions.


Applications:

Exstruded and co-exstruded sheets, including thick sheet where high hot draw ratios are required.
Its excellent surface appearance permit the use in a wide range of applications such as furniture, refrigerator, sanitary, automotive and packaging for foodstuff and industrial items.
Also ideal for the extrusion of profiles for furniture industry.

 

加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 4 cm³/10min ISO 1133
温度 220 °C -
载荷 10 kg -
熔体密度 960 kg/m³ -
熔体的比热 2150 J/(kg K) -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2300 MPa ISO 527
屈服应力 45 MPa ISO 527
屈服伸长率 3 % ISO 527
名义断裂伸长率 30 % ISO 527
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 140 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 18 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 8 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
玻璃化转变温度, 10°C/min 109 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 83 °C ISO 75-1/-2
维卡软化温度, B 104 °C ISO 306
线性热膨胀系数, 平行 90 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
Yellow Card 现存 是的 - -
电性能价值单位Test Standard
ISO数据
相对介电常数., 1MHz 3.1 - IEC 62631-2-1
介质损耗因子, 1MHz 150 E-4 IEC 62631-2-1
体积电阻率 1E13 Ohm*m IEC 62631-3-1
表面电阻率 1E14 Ohm IEC 62631-3-2
介电强度 30 kV/mm IEC 60243-1
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
吸水性 0.6 % 类似ISO 62
吸湿性 0.2 % 类似ISO 62
密度 1040 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
ISO试样制备条件. 2580 - ISO ....-2
注塑, 熔体温度 250 °C ISO 294
注塑, 模具温度 60 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
注塑, 保压压力 70 MPa ISO 294
函数
粘度-剪切速度 , SINKRAL® B4 Milano, ABS, Versalis
剪切应力-剪切速度 , SINKRAL® B4 Milano, ABS, Versalis
动态剪切模量-温度 , SINKRAL® B4 Milano, ABS, Versalis
应力-应变.  , SINKRAL® B4 Milano, ABS, Versalis
正割模量-应变.  , SINKRAL® B4 Milano, ABS, Versalis
比容-温度(pvT) , SINKRAL® B4 Milano, ABS, Versalis
单位质量比焓-温度(DSC) , SINKRAL® B4 Milano, ABS, Versalis
典型数据
加工方法
薄膜挤出成型, 异型材挤出成型, 片材挤出成型, 其它挤出成型, 吹塑, 热成型
供货形式
粒料
特殊性能
经热稳处理的/耐热的
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
薄膜挤出成型
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

  Typical processing temperature range:

    Melt temperature           190 - 230 °C

其E烦龀尚
Other  extrusion
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

E尾募烦龀尚
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

板材挤出成型
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.