Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Spectar™ - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Spectar™:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Spectar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastman Spectar™ Clear is a copolyester, developed by Eastman to achieve measurably improved sheet clarity and edge color while maintaining the performance characteristics for which Eastman Spectar™ copolyester has become known in the industry. It offers the thermoformability and ease of fabrication of Eastman Spectar™ copolyester along with significantly improved clarity. Eastman Spectar™ Clear also offers approximately double the notch impact strength, 50% higher instrumented impact strength and better chemical resistance when compared

to traditional Spectar™ Copolyester.




机械性能价值单位Test Standard
ASTM数据
拉伸模量 1800 MPa ASTM D 638
屈服应力 48 MPa ASTM D 638
断裂拉伸强度 53 MPa ASTM D 638
屈服伸长率 5 % ASTM D 638
断裂伸长率 340 % ASTM D 638
弯曲模量 2000 MPa ASTM D 790
洛克硬度 R 107 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in N J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 83 J/m ASTM D 256
温度 -30 °C -
Izod冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
UL94 燃烧性 HB - UL 94
热释放速率, 平行 76.2 E-6/K ASTM D 696
DTUL @ 66 psi 77 °C ASTM D 648
DTUL @ 264 psi 73 °C ASTM D 648
维卡温度 86 °C ASTM D 1525
电性能价值单位Test Standard
ASTM数据
表面电阻率 1E17 Ohm ASTM D 257
体积电阻率 1E16 Ohm*cm ASTM D 257
耐电弧性 130 s ASTM D 495
光学特性价值单位Test Standard
ASTM数据
光泽度 150 - ASTM D 2457
雾度 0.5 % ASTM D 1003
光透射率 91 % ASTM D 1003
其它性能价值单位Test Standard
吸水率, 24小时 0.19 % ASTM D 570
密度 1230 kg/m³ ASTM D 792
典型数据
加工方法
片材挤出成型, 热成型
特殊性能
高冲击韧性的/经抗冲改性的, 透明.
特征
少气味, 共聚物
耐化学试剂
通用耐化学性
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com