Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS ECO 440 FC MR100 - PS-I - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS ECO 440 FC MR100:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Styrolution® PS ECO 440FC MR100 is a mechanically recycled high impact polystyrene grade containing 100%

recycled material.

Styrolution® PS ECO 440FC MR100 is a mechanically recycled high impact polystyrene grade containing 100% recycled material.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 6 cm³/10min ISO 1133
温度 200 °C -
载荷 5 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2000 MPa ISO 527
屈服应力 23 MPa ISO 527
屈服伸长率 1.5 % ISO 527
名义断裂伸长率 32 % ISO 527
弯曲模量, 23°C 1900 MPa ISO 178
简支梁缺口冲击强度, +23°C 8 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
维卡软化温度, B 89 °C ISO 306
ASTM数据
维卡温度 89 °C ASTM D 1525
其它性能价值单位Test Standard
Recycled resin content 100 % -
加工推荐(注塑)价值单位Test Standard
注塑熔体温度 180 - 260 °C -
加工推荐(挤出)价值单位Test Standard
注塑熔体温度 180 - 240 °C -
典型数据
加工方法
注塑, 薄膜挤出成型, 异型材挤出成型, 片材挤出成型, 其它挤出成型
供货形式
粒料, 白色
特殊性能
高冲击韧性的/经抗冲改性的
Certifications
回收树脂含量, 可食品接触的
应用
电子电气, 包装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
PROCESSING

Injection molding, Melt temperature, range: 180 - 260°C

Styrolution® PS ECO 440FC MR100 can be injection molded under different conditions depending on machinery available and articles molded. Mass temperature can be as high as 260°C. To achieve articles with very high gloss, well-polished surfaces are recommended.

薄膜挤出成型
VERARBEITUNG

Schlauchfolien Massetemperatur: 180 - 210°C

Flachfolien Massetemperatur: 200 - 240°C

Die Massetemperatur in der Extrusion sollte 240°C nicht überschreiten.

其E烦龀尚
PROCESSING

Pipes, Melt temperature: 180 - 210°C

E尾募烦龀尚
PROCESSING

Profiles, Melt temperature: 210°C

板材挤出成型
PROCESSING

Plates, Melt temperature: 200 - 230°C

权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.