Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of STYRON X-TECH™ 2175 - (PS-HI) - Trinseo

Material Data Center offers the following functions for STYRON X-TECH™ 2175:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Styron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 2.6 g/10min ISO 1133
温度 200 °C -
负载 5 kg -
ASTM数据
熔融指数, MFI 2.6 g/10min ASTM D 1238
温度 200 °C -
负载 5 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 1700 MPa ISO 527
屈服应力 16 MPa ISO 527
断裂应力 26 MPa ISO 527
断裂伸长率 63 % ISO 527
弯曲模量, 23°C 1800 MPa ISO 178
弯曲强度 37 MPa ISO 178
简支梁缺口冲击强度, +23°C 9.1 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 6.6 kJ/m² ISO 179/1eA
ASTM数据
拉伸模量 1700 MPa ASTM D 638
屈服应力 16 MPa ASTM D 638
断裂拉伸强度 26 MPa ASTM D 638
断裂伸长率 63 % ASTM D 638
弯曲模量 1800 MPa ASTM D 790
弯曲强度 37 MPa ASTM D 790
悬臂梁缺口冲击强度, 1/8 in 82 J/m ASTM D 256
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 69 °C ISO 75-1/-2
热变形温度, 0.45 MPa 82 °C ISO 75-1/-2
维卡软化温度, A 99 °C ISO 306
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
ASTM数据
DTUL @ 66 psi 82 °C ASTM D 648
DTUL @ 264 psi 69 °C ASTM D 648
维卡温度 99 °C ASTM D 1525
其它性能价值单位Test Standard
密度 1050 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
密度 1050 kg/m³ ASTM D 792
典型数据
加工方法
片材挤出成型, 其它挤出成型, 热成型
特殊性能
高冲击韧性的/经抗冲改性的
特征
熔体强度
耐化学试剂
耐环境应力裂纹性
Certifications
可食品接触的, 10/2011认证, FDA 21 CFR认证
应用
制冷
地区供应
欧洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com