Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SUPREME SP 6720 - SMMA - Supreme Petrochem Ltd

Material Data Center offers the following functions for SUPREME SP 6720:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Supreme datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
熔融指数, MFI 4 g/10min ASTM D 1238
温度 200 °C -
负载 5 kg -
模压收缩率, 平行 0.004 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
屈服应力 42.2 MPa ASTM D 638
弯曲模量 2482 MPa ASTM D 790
弯曲强度 67.2 MPa ASTM D 790
悬臂梁缺口冲击强度, 1/8 in 30 J/m ASTM D 256
Izod冲击强度, 1/8 in 250 J/m ASTM D 256
Other Standards[S]
洛克硬度 R 55 -
S: These properties are reported by the producer according standards that are different to our defaults.
热性能价值单位Test Standard
ASTM数据
UL94 燃烧性 HB - UL 94
测试厚度 1.6 mm -
DTUL @ 264 psi 82 °C ASTM D 648
维卡温度 90 °C ASTM D 1525
光学特性价值单位Test Standard
ASTM数据
雾度 1.5 % ASTM D 1003
其它性能价值单位Test Standard
密度 1050 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 °C -
预干燥-时间 1 h -
注塑熔体温度 180 - 240 °C -
模具温度 50 - 70 °C -
典型数据
加工方法
注塑, 热成型
供货形式
粒料
特殊性能
透明.
特征
High Gloss
Certifications
可食品接触的, FDA 21 CFR认证, RoHS
应用
IT/商务机器, 包装
地区供应
中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.