Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Teflon™ PFA 345 - PFA - The Chemours Company

Material Data Center offers the following functions for Teflon™ PFA 345:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Teflon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
Other Standards[S]
熔融指数, MFI 5 g/10min ASTM D 3307
S: These properties are reported by the producer according standards that are different to our defaults.
机械性能价值单位Test Standard
ASTM数据
弯曲模量 551 MPa ASTM D 790
邵氏硬度D 55 - ASTM D 2240
Other Standards[S]
拉伸强度 27 MPa ASTM D 3307
断裂伸长率 300 % ASTM D 3307
S: These properties are reported by the producer according standards that are different to our defaults.
热性能价值单位Test Standard
ASTM数据
UL94 燃烧性 V-0 - UL 94
氧指数 95 % ASTM D 2863
Other Standards[S]
熔点 305 °C ASTM D 4591
最高工作温度, 长期 260 °C -
S: These properties are reported by the producer according standards that are different to our defaults.
电性能价值单位Test Standard
ASTM数据
电介质强度, 短时 80 kV/mm ASTM D 149
耗散因素, 1 MHz 0.0002 - ASTM D 150
电介质常数, 1 MHz 2.03 - ASTM D 150
体积电阻率 1E18 Ohm*cm ASTM D 257
其它性能价值单位Test Standard
吸水率, 24小时 0.03 % ASTM D 570
密度 2150 kg/m³ ASTM D 792
典型数据
加工方法
注塑, 管材挤出, 电线挤出, 其它挤出成型, 模压/烧结成型, 模压成型
供货形式
粒料
特殊性能
经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
特征
防蠕变, Good Drawdown, 低烟量, 熔体强度, 热稳定性, Tribologic Grade
耐化学试剂
通用耐化学性, 耐环境应力裂纹性
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.