Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Terluran® HI-10 - ABS - INEOS Styrolution

Material Data Center offers the following functions for Terluran® HI-10:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Terluran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
High impact grade, suitable for injection moulding and extrusion.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 5.5 cm³/10min ISO 1133
温度 220 °C -
载荷 10 kg -
喷射温度 102 °C -
机械性能价值单位Test Standard
ISO数据
拉伸模量 1900 MPa ISO 527
屈服应力 38 MPa ISO 527
屈服伸长率 2.8 % ISO 527
名义断裂伸长率 9 % ISO 527
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 140 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 35 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 13 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 93 °C ISO 75-1/-2
热变形温度, 0.45 MPa 97 °C ISO 75-1/-2
维卡软化温度, B 90 °C ISO 306
线性热膨胀系数, 平行 95 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 2.9 - IEC 62631-2-1
相对介电常数., 1MHz 2.8 - IEC 62631-2-1
介质损耗因子, 100Hz 54 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 82 E-4 IEC 62631-2-1
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
表面电阻率 1E13 Ohm IEC 62631-3-2
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
吸水性 1.03 % 类似ISO 62
吸湿性 0.21 % 类似ISO 62
密度 1030 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 250 °C ISO 294
注塑, 模具温度 60 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
函数
粘度-剪切速度 , Terluran® HI-10, ABS, INEOS Styrolution
剪切应力-剪切速度 , Terluran® HI-10, ABS, INEOS Styrolution
应力-应变.  , Terluran® HI-10, ABS, INEOS Styrolution
正割模量-应变.  , Terluran® HI-10, ABS, INEOS Styrolution
应力-应变(等时的) 23°C, Terluran® HI-10, ABS, INEOS Styrolution
蠕变模量-时间. 23°C, Terluran® HI-10, ABS, INEOS Styrolution
蠕变曲线 23°C, Terluran® HI-10, ABS, INEOS Styrolution
应力-应变(等时的) 60°C, Terluran® HI-10, ABS, INEOS Styrolution
蠕变模量-时间. 60°C, Terluran® HI-10, ABS, INEOS Styrolution
蠕变曲线 60°C, Terluran® HI-10, ABS, INEOS Styrolution
比容-温度(pvT) , Terluran® HI-10, ABS, INEOS Styrolution
拉伸模量-温度 , Terluran® HI-10, ABS, INEOS Styrolution
典型数据
加工方法
注塑, 异型材挤出成型, 片材挤出成型, 其它挤出成型
供货形式
粒料
地区供应
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
injection molding, Melt temperature, range: 230 - 260 °C
injection molding, Melt temperature, recommended: 250 °C
injection molding, Mold temperature, range: 30 - 60 °C
injection molding, Mold temperature, recommended: 50 °C
其E烦龀尚
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
Extrusion, Pipes, Melt temperature: 200 - 230 °C
E尾募烦龀尚
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
Extrusion, Profiles, Melt temperature: 230 °C
板材挤出成型
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
Extrusion, Plates, Melt temperature: 210 - 240 °C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.