Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of THERMOLAST® M TM4MED - TPE - KRAIBURG TPE GmbH & Co. KG

Material Data Center offers the following functions for THERMOLAST® M TM4MED:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Thermolast datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Typical Markets/ Application Sectors:
•    Medical application

Application Examples:
•    Seals
•    Mouthpieces
•    Valves
•    Soft touch
•    Flexible connections
•    Medical tubes

Material Advantage:
•    Applicaton up to indirect blood contact
•    Tested acord. USP Class IV and ISO 10993-5
•    Tested according to ISO 10993-11, ISO 10993- 10, USP 6.6.1
•    Adhesion to PP und HDPE
•    Adapted for injection moulding and extrusion
•    Very good compression set
•    sterilizable (autoclave 134°C, gammaradiation 2x35 kGy, EtO)
机械性能价值单位Test Standard
ISO数据
拉伸强度 8 MPa ISO 37
断裂伸长率 800 % ISO 37
70°C时恒定应变下的永久变形, 24h 26 % ISO 815
100°C时恒定应变下的永久变形, 24h 43 % ISO 815
撕裂强度 11.5 kN/m ISO 34-1
肖氏硬度A 36 - ISO 7619-1
其它性能价值单位Test Standard
密度 880 kg/m³ ISO 1183
加工推荐(注塑)价值单位Test Standard
预干燥-温度 60 - 80 °C -
预干燥-时间 2 - 4 h -
注塑熔体温度 200 - 250 °C -
模具温度 25 - 40 °C -
1区 180 - 200 °C -
2区 200 - 220 °C -
3区 220 - 250 °C -
注射压力 20 - 100 MPa -
背压 2 - 10 MPa -
保压压力 8 - 60 MPa -
最大停留时间 10 min -
典型数据
加工方法
注塑, 其它挤出成型
特殊性能
Translucent, 消毒, 环氧乙烷灭菌(EtO), 蒸汽灭菌, Gamma irradiation sterilization
特征
好粘附性能, 软质, 可焊的
耐化学试剂
抗辐射性
Certifications
医用级, Biocompatibility ISO 10993, US药物六级认证, Drug Master File, Long term supply assurance, RoHS, REACH
应用
药物
地区供应
北美, 欧洲, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.