Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Treva™ GC6011NAT - CAP - Eastman Chemical Co.

Material Data Center offers the following functions for Treva™ GC6011NAT:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Treva datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastman TREVA™ is a cellulose-based engineering bioplastic that offers both high performance and enables exceptional depth of color and high gloss for opaque applications. TREVA is chemically resistant, dimensionally stable and has excellent flow, BPA-free and enables exceptional depth of color and high gloss for opaque

applications.

加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.007 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
屈服应力 55 MPa ASTM D 638
断裂拉伸强度 51 MPa ASTM D 638
断裂伸长率 21 % ASTM D 638
弯曲模量 2160 MPa ASTM D 790
洛克硬度 R 108 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 82 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 66 J/m ASTM D 256
温度 -40 °C -
热性能价值单位Test Standard
ASTM数据
DTUL @ 66 psi 116 °C ASTM D 648
DTUL @ 264 psi 102 °C ASTM D 648
维卡温度 131 °C ASTM D 1525
其它性能价值单位Test Standard
Biobased content 45 % -
吸水率, 24小时 2.3 % ASTM D 570
密度 1230 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 75 °C -
预干燥-时间 4 h -
注塑熔体温度 260 °C -
模具温度 85 °C -
注射速度 30 mm/s -
最大停留时间 4 min -
典型数据
加工方法
注塑
供货形式
自然色
特殊性能
Opaque
特征
High Gloss, 低双折射率
耐化学试剂
通用耐化学性
Certifications
生物相容
应用
包装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.