Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ FX100 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ FX100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastman Tritan™ FX100 is a copolyester resin for extruded film applications where enhanced heat resistance and toughness are required. It works great in high temperature packaging, transaction and identification cards, and

protective laminates.

Packaging brands and film converters prefer Tritan™ FX100 for its ability to provide a clear, aesthetically pleasing package that stands up to the strenuous requirements for hot filling, while also providing safety that consumers expect. It’s great for brands looking to replace materials of concern or premiumize their packaging by transitioning from opaque to clear.

Transaction and identification card producers, brands, and governments alike value Tritan™ FX100 for its excellent bend strength and chemical resistance, which provides longer useful life and better security. Compared to PVC and other material alternatives. Transaction cards made with Tritan™ have been found to withstand more than 10 times the number of flexural cycles using industry standard fitness for use testing protocols.

Tritan™ FX100 may be used in various food contact applications under the U.S. Food & Drug Administration (FDA) regulations.

热性能价值单位Test Standard
ASTM数据
热释放速率, 平行 90 E-6/K ASTM D 696
玻璃化转变温度 110 °C ASTM E 1356
光学特性价值单位Test Standard
ASTM数据
光泽度 161 - ASTM D 2457
雾度 0.7 % ASTM D 1003
光透射率 92 % ASTM D 1003
折射率 1.55 - ASTM D 542
其它性能价值单位Test Standard
吸水率, 24小时 0.5 % ASTM D 570
密度 1190 kg/m³ ASTM D 792
机械性能(薄膜)价值单位Test Standard
ISO数据
继续撕裂强度, 平行 11 N/mm ISO 6383-1
继续撕裂强度, 垂直 11 N/mm ISO 6383-1
试样厚度 0.254 mm -
ASTM Data
拉伸模量, 平行 1500 MPa ASTM D 882
拉伸模量, 垂直 1400 MPa ASTM D 882
屈服应力, 平行 41 MPa ASTM D 882
屈服应力, 垂直 40 MPa ASTM D 882
断裂拉伸强度, 平行 59 MPa ASTM D 882
断裂拉伸强度, 垂直 52 MPa ASTM D 882
屈服伸长率, 平行 7 % ASTM D 882
屈服伸长率, 垂直 7 % ASTM D 882
断裂伸长率, 平行 179 % ASTM D 882
断裂伸长率, 垂直 203 % ASTM D 882
试样厚度 0.254 mm -
典型数据
加工方法
其它挤出成型
特殊性能
经热稳处理的/耐热的, 透明.
特征
无定形, High Gloss, 抗划性, 共聚物
耐化学试剂
通用耐化学性
Certifications
可食品接触的, FDA 21 CFR认证
应用
包装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.