Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ MP100 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ MP100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastman Tritan™ MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation copolyester can be thermoformed with a wide processing window that allows for product designs that reflect intricate detail.

Eastman Tritan™ MP100 copolyester is suitable for use with most forms of sterilization including radiation and ethylene oxide. It is NOT suitable for autoclave/steam sterilization. Eastman Tritan™ MP100 copolyester has been

formulated for use in medical film, sheet, and packaging applications.

热性能价值单位Test Standard
ASTM数据
热释放速率, 平行 88 E-6/K ASTM D 696
玻璃化转变温度 110 °C ASTM E 1356
光学特性价值单位Test Standard
ASTM数据
光泽度 161 - ASTM D 2457
雾度 1 % ASTM D 1003
光透射率 92 % ASTM D 1003
折射率 1.54 - ASTM D 542
其它性能价值单位Test Standard
吸水率, 24小时 0.5 % ASTM D 570
密度 1190 kg/m³ ASTM D 792
机械性能(薄膜)价值单位Test Standard
ISO数据
继续撕裂强度, 平行 11 N/mm ISO 6383-1
继续撕裂强度, 垂直 11 N/mm ISO 6383-1
试样厚度 0.25 mm -
ASTM Data
拉伸模量, 平行 1460 MPa ASTM D 882
拉伸模量, 垂直 1380 MPa ASTM D 882
屈服应力, 平行 41 MPa ASTM D 882
屈服应力, 垂直 40 MPa ASTM D 882
断裂拉伸强度, 平行 59 MPa ASTM D 882
断裂拉伸强度, 垂直 52 MPa ASTM D 882
屈服伸长率, 平行 7 % ASTM D 882
屈服伸长率, 垂直 7 % ASTM D 882
断裂伸长率, 平行 179 % ASTM D 882
断裂伸长率, 垂直 203 % ASTM D 882
试样厚度 0.25 mm -
典型数据
加工方法
薄膜挤出成型, 片材挤出成型, 热成型
特殊性能
经热稳处理的/耐热的, 透明., 消毒, 环氧乙烷灭菌(EtO), Gamma irradiation sterilization
特征
无定形, 可热封的, 共聚物
耐化学试剂
通用耐化学性, 抗辐射性
应用
药物, 包装
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.