Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ MP150 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ MP150:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastman Tritan copolyester MP150 is a high flow grade of Eastman Tritan. Eastman Tritan copolyester MP150 has viscosity reductions of 40-50% relative to Eastman Tritan copolyester MP100. It is intended for use in extrusion coating processes or where high melt flow rate is desirable.

Other outstanding features include good toughness, hydrolytic stability, and heat and chemical resistance.

Eastman Tritan copolyester MP150 may be used in food contact applications with restrictions and is compliant with applicable and select sections of USP 35 <661>, ISO10993, and ISO11607.

加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.006 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
拉伸模量 1575 MPa ASTM D 638
屈服应力 43 MPa ASTM D 638
断裂拉伸强度 52 MPa ASTM D 638
屈服伸长率 7 % ASTM D 638
断裂伸长率 210 % ASTM D 638
弯曲模量 1575 MPa ASTM D 790
洛克硬度 R 111 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 860 J/m ASTM D 256
Izod冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
DTUL @ 66 psi 94 °C ASTM D 648
DTUL @ 264 psi 81 °C ASTM D 648
玻璃化转变温度 110 °C ASTM E 1356
光学特性价值单位Test Standard
ASTM数据
雾度 1 % ASTM D 1003
光透射率 91 % ASTM D 1003
其它性能价值单位Test Standard
密度 1180 kg/m³ ASTM D 792
机械性能(薄膜)价值单位Test Standard
ASTM Data
拉伸模量, 平行 979 MPa ASTM D 882
断裂拉伸强度, 平行 56.5 MPa ASTM D 882
断裂伸长率, 平行 217 % ASTM D 882
试样厚度 0.127 mm -
加工推荐(挤出)价值单位Test Standard
预干燥-温度 88 °C -
预干燥-时间 4 - 6 h -
注塑熔体温度 260 - 282 °C -
模具温度 38 - 66 °C -
典型数据
加工方法
表面涂层, 热成型
特殊性能
经热稳处理的/耐热的, 透明.
特征
共聚物
耐化学试剂
通用耐化学性, 水解稳定
Certifications
可食品接触的, 医用级, Biocompatibility ISO 10993, US药物六级认证
应用
药物, 包装
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.