Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ MXF321-19164FC ST - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ MXF321-19164FC ST:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastman Tritan MXF321 copolyester has been formulated for medical devices and meets UL94 V2 compliance at 1.5 mm. Eastman Tritan MXF321 has passed ISO 10993 testing for cytotoxicity, skin sensitization, and intracutaneous reactivity. Tritan MXF321 has many outstanding features that include excellent toughness,

hydrolytic stability, heat resistance, chemical resistance, and melt flowability. Eastman Tritan MXF321 contains a mold release derived from vegetable based sources.

加工/物理特性价值单位Test Standard
ASTM数据
熔融指数, MFI 11 g/10min ASTM D 1238
温度 260 °C -
负载 2.16 kg -
模压收缩率, 平行 0.0045 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
拉伸模量 1850 MPa ASTM D 638
屈服应力 49 MPa ASTM D 638
断裂伸长率 50 % ASTM D 638
悬臂梁缺口冲击强度, 1/8 in 1100 J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
UL94 燃烧性 V-2 - UL 94
测试厚度 1.5 mm -
DTUL @ 66 psi 76 °C ASTM D 648
DTUL @ 264 psi 66 °C ASTM D 648
其它性能价值单位Test Standard
密度 1200 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 °C -
预干燥-时间 4 - 6 h -
注塑熔体温度 260 - 280 °C -
模具温度 18 - 50 °C -
典型数据
加工方法
注塑
供货形式
白色
添加剂
脱模助剂
特殊性能
经热稳处理的/耐热的
特征
共聚物
耐化学试剂
通用耐化学性, 水解稳定
Certifications
医用级, Biocompatibility ISO 10993
应用
药物
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.