Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 6550 FC / PBT 6550 - PBT - BASF

Material Data Center offers the following functions for Ultradur® B 6550 FC / PBT 6550:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulations including FDA, European Food Contact (EU) Nr. 10/2011 and GMP (EC) N°2023/2006.

Additional food contact compliances may also be available. Please contact your local representative or plastics safety (E-Mail: plastics.safety@basf.com).

Abbreviated designation according to ISO 1043-1: PBT
CLASSIFICATION ACCORDING TO ISO 7792-1:
Moulding Compound ISO 7792-PBT, EGHLN, 15-020
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 9 cm³/10min ISO 1133
温度 250 °C -
载荷 2.16 kg -
模塑收缩率, 平行 1.7 % ISO 294-4, 2577
模塑收缩率, 垂直 2.1 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 2400 MPa ISO 527
屈服应力 54 MPa ISO 527
屈服伸长率 3.5 % ISO 527
名义断裂伸长率 >50 % ISO 527
拉伸蠕变模量, 1h 1800 MPa ISO 899-1
拉伸蠕变模量, 1000h 1100 MPa ISO 899-1
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 6 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 223 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 55 °C ISO 75-1/-2
热变形温度, 0.45 MPa 135 °C ISO 75-1/-2
线性热膨胀系数, 平行 110 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 110 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 3.3 - IEC 62631-2-1
相对介电常数., 1MHz 3.3 - IEC 62631-2-1
介质损耗因子, 100Hz 10 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 200 E-4 IEC 62631-2-1
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
表面电阻率 1E13 Ohm IEC 62631-3-2
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
吸水性 0.5 % 类似ISO 62
吸湿性 0.25 % 类似ISO 62
密度 1300 kg/m³ ISO 1183
模塑测量的特殊性能价值单位Test Standard
ISO数据
粘数 160 cm³/g ISO 307, 1157, 1628
函数
粘度-剪切速度 , Ultradur® B 6550 FC / PBT 6550, PBT, BASF
剪切应力-剪切速度 , Ultradur® B 6550 FC / PBT 6550, PBT, BASF
应力-应变.  , Ultradur® B 6550 FC / PBT 6550, PBT, BASF
正割模量-应变.  , Ultradur® B 6550 FC / PBT 6550, PBT, BASF
应力-应变(等时的) 23°C, Ultradur® B 6550 FC / PBT 6550, PBT, BASF
蠕变模量-时间. 23°C, Ultradur® B 6550 FC / PBT 6550, PBT, BASF
蠕变曲线 23°C, Ultradur® B 6550 FC / PBT 6550, PBT, BASF
拉伸模量-温度 , Ultradur® B 6550 FC / PBT 6550, PBT, BASF
典型数据
加工方法
注塑, 薄膜挤出成型, 异型材挤出成型, 片材挤出成型, 其它挤出成型
供货形式
粒料
Certifications
可食品接触的, 10/2011认证, FDA 21 CFR认证
地区供应
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
injection molding, Dwell time, thermoplastics: 10 min
其E烦龀尚
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Prepreg, Melt temperature: 230 - 250 °C
Extrusion, Pipes, Melt temperature: 230 - 260 °C
Extrusion, cable sheathing, Melt temperature: 230 - 260 °C
E尾募烦龀尚
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Profiles, Melt temperature: 230 - 260 °C
板材挤出成型
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
injection molding, Dwell time, thermoplastics: 10 min
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.