Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 1523 FC R01 - PBT - BASF

Material Data Center offers the following functions for Ultradur® B 1523 FC R01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Ultradur® B1523 FC R01 UN is suitable for plastic parts, where material approval regarding direct food contact is a mandatory requirement.

The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulations including European Food Contact (EU) Nr. 10/2011 and GMP (EC) N°2023/2006.

For questions regarding the compliance with further regulations, and certificates, please contact your local BASF representative or Plastics Safety (E-Mail: plastics.safety@basf.com).

The products can also be offered as BMBcert™ and/or Ccycled™. Due to the Massbalance approach the product properties do not change.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 90 cm³/10min ISO 1133
温度 250 °C -
载荷 2.16 kg -
模塑收缩率, 平行 2.0 % ISO 294-4, 2577
模塑收缩率, 垂直 2.2 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 1600 MPa ISO 527
屈服应力 43 MPa ISO 527
屈服伸长率 10 % ISO 527
名义断裂伸长率 20 % ISO 527
无缺口简支梁冲击强度, +23°C 225 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 75 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 5 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 2.5 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 224 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 55 °C ISO 75-1/-2
热变形温度, 0.45 MPa 145 °C ISO 75-1/-2
维卡软化温度, B 150 °C ISO 306
线性热膨胀系数, 平行 140 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 140 E-6/K ISO 11359-1/-2
其它性能价值单位Test Standard
密度 1300 kg/m³ ISO 1183
模塑测量的特殊性能价值单位Test Standard
ISO数据
粘数 100 cm³/g ISO 307, 1157, 1628
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 - 120 °C -
预干燥-时间 4 h -
加工湿度 ≤0.04 % -
注塑熔体温度 260 - 280 °C -
模具温度 20 - 60 °C -
典型数据
Certifications
可食品接触的, 10/2011认证
地区供应
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 260 - 280 °C
injection molding, Melt temperature, recommended: 275 °C
injection molding, Mold temperature, range: 20 - 60 °C
injection molding, Mold temperature, recommended: 40 °C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.