Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 4500 - PBT - BASF

Material Data Center offers the following functions for Ultradur® B 4500:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
中等黏度规格,可用于注塑,挤出流延膜及薄壁型材和管材的技术应用

根据ISO1043-1分类规则:PBT
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 19 cm³/10min ISO 1133
温度 250 °C -
载荷 2.16 kg -
模塑收缩率, 平行 1.6 % ISO 294-4, 2577
模塑收缩率, 垂直 1.9 % ISO 294-4, 2577
ASTM数据
模压收缩率, 平行 0.015 mm/mm ASTM D 955
机械性能价值单位Test Standard
ISO数据
拉伸模量 2500 MPa ISO 527
屈服应力 55 MPa ISO 527
屈服伸长率 3.7 % ISO 527
名义断裂伸长率 >50 % ISO 527
拉伸蠕变模量, 1h 1800 MPa ISO 899-1
拉伸蠕变模量, 1000h 1200 MPa ISO 899-1
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 180 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 5 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 4 kJ/m² ISO 179/1eA
ASTM数据
拉伸模量 2620 MPa ASTM D 638
屈服应力 60 MPa ASTM D 638
屈服伸长率 3.7 % ASTM D 638
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 223 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 65 °C ISO 75-1/-2
热变形温度, 0.45 MPa 165 °C ISO 75-1/-2
线性热膨胀系数, 平行 110 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 110 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
Yellow Card 现存 是的 - -
燃烧性-氧指数 20 % ISO 4589-1/-2
ASTM数据
DTUL @ 66 psi 164 °C ASTM D 648
DTUL @ 264 psi 66.1 °C ASTM D 648
熔点 223 °C ASTM D 3418
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 3.3 - IEC 62631-2-1
相对介电常数., 1MHz 3.3 - IEC 62631-2-1
介质损耗因子, 100Hz 10 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 200 E-4 IEC 62631-2-1
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
表面电阻率 1E13 Ohm IEC 62631-3-2
介电强度 36 kV/mm IEC 60243-1
相对漏电起痕指数 550 - IEC 60112
其它性能价值单位Test Standard
吸水性 0.5 % 类似ISO 62
吸湿性 0.25 % 类似ISO 62
密度 1300 kg/m³ ISO 1183
密度 1680 kg/m³ ASTM D 792
模塑测量的特殊性能价值单位Test Standard
ISO数据
粘数 130 cm³/g ISO 307, 1157, 1628
加工推荐(注塑)价值单位Test Standard
预干燥-温度 80 - 120 °C -
预干燥-时间 4 h -
加工湿度 ≤0.04 % -
注塑熔体温度 250 - 275 °C -
模具温度 40 - 70 °C -
函数
粘度-剪切速度 , Ultradur® B 4500, PBT, BASF
剪切应力-剪切速度 , Ultradur® B 4500, PBT, BASF
应力-应变.  , Ultradur® B 4500, PBT, BASF
正割模量-应变.  , Ultradur® B 4500, PBT, BASF
应力-应变(等时的) 23°C, Ultradur® B 4500, PBT, BASF
蠕变模量-时间. 23°C, Ultradur® B 4500, PBT, BASF
蠕变曲线 23°C, Ultradur® B 4500, PBT, BASF
应力-应变(等时的) 40°C, Ultradur® B 4500, PBT, BASF
蠕变模量-时间. 40°C, Ultradur® B 4500, PBT, BASF
蠕变曲线 40°C, Ultradur® B 4500, PBT, BASF
应力-应变(等时的) 60°C, Ultradur® B 4500, PBT, BASF
蠕变模量-时间. 60°C, Ultradur® B 4500, PBT, BASF
蠕变曲线 60°C, Ultradur® B 4500, PBT, BASF
拉伸模量-温度 , Ultradur® B 4500, PBT, BASF
典型数据
加工方法
注塑, 薄膜挤出成型, 异型材挤出成型, 其它挤出成型
供货形式
粒料, 自然色
特殊性能
经光稳处理的/耐光的, 经耐紫外线处理的/耐气候的, 经热稳处理的/耐热的
地区供应
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 70 °C
injection molding, Mold temperature, recommended: 60 °C
薄膜挤出成型
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Flat film, Melt temperature: 230 - 280 °C
其E烦龀尚
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Prepreg, Melt temperature: 230 - 250 °C
Extrusion, Pipes, Melt temperature: 230 - 260 °C
E尾募烦龀尚
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 70 °C
injection molding, Mold temperature, recommended: 60 °C
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.