Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® N2720 M210 AT - POM-MD10 - BASF

Material Data Center offers the following functions for Ultraform® N2720 M210 AT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Grade with enhanced stiffness and strength as well as good wear properties, e.g. used for conveyor belts and transportation systems.

Abbreviated designation according to ISO 1043: POM-MD
Designation according to ISO 29988-POM-K,MD,M-GNRS2,3-2
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 7 cm³/10min ISO 1133
温度 190 °C -
载荷 2.16 kg -
模塑收缩率, 平行 1.7 % ISO 294-4, 2577
模塑收缩率, 垂直 1.9 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 3800 MPa ISO 527
屈服应力 63 MPa ISO 527
屈服伸长率 9.5 % ISO 527
名义断裂伸长率 18 % ISO 527
无缺口简支梁冲击强度, +23°C 90 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 90 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 3.5 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 3.5 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 166 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 115 °C ISO 75-1/-2
维卡软化温度, B 150 °C ISO 306
线性热膨胀系数, 平行 80 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.6 mm -
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 3.2 mm -
Yellow Card 现存 是的 - -
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 3.9 - IEC 62631-2-1
相对介电常数., 1MHz 3.8 - IEC 62631-2-1
介质损耗因子, 100Hz 50 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 60 E-4 IEC 62631-2-1
体积电阻率 1E10 Ohm*m IEC 62631-3-1
表面电阻率 1E14 Ohm IEC 62631-3-2
介电强度 40 kV/mm IEC 60243-1
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
吸水性 0.8 % 类似ISO 62
吸湿性 0.2 % 类似ISO 62
密度 1490 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 200 °C ISO 294
注塑, 模具温度 90 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
加工推荐(注塑)价值单位Test Standard
预干燥-温度 100 °C -
预干燥-时间 3 h -
加工湿度 ≤0.2 % -
注塑熔体温度 190 - 230 °C -
模具温度 60 - 120 °C -
函数
应力-应变.  , Ultraform® N2720 M210 AT, POM-MD10, BASF
正割模量-应变.  , Ultraform® N2720 M210 AT, POM-MD10, BASF
应力-应变(等时的) 23°C, Ultraform® N2720 M210 AT, POM-MD10, BASF
蠕变模量-时间. 23°C, Ultraform® N2720 M210 AT, POM-MD10, BASF
蠕变曲线 23°C, Ultraform® N2720 M210 AT, POM-MD10, BASF
应力-应变(等时的) 60°C, Ultraform® N2720 M210 AT, POM-MD10, BASF
蠕变模量-时间. 60°C, Ultraform® N2720 M210 AT, POM-MD10, BASF
蠕变曲线 60°C, Ultraform® N2720 M210 AT, POM-MD10, BASF
应力-应变(等时的) 120°C, Ultraform® N2720 M210 AT, POM-MD10, BASF
蠕变模量-时间. 120°C, Ultraform® N2720 M210 AT, POM-MD10, BASF
蠕变曲线 120°C, Ultraform® N2720 M210 AT, POM-MD10, BASF
拉伸模量-温度 , Ultraform® N2720 M210 AT, POM-MD10, BASF
典型数据
加工方法
注塑
供货形式
粒料
添加剂
润滑剂
特征
共聚物
地区供应
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 190 - 230 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 60 - 120 °C
injection molding, Mold temperature, recommended: 90 °C
injection molding, Dwell time, thermoplastics: 10 min

Processing

Usual single-flighted three-section screws with an effective screw length of at least 15 D, better 20 - 23 D are suitable for the injection molding of Ultraform.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.


Postprocessing

If parts were produced at a comparatively low mold temperature (e.g. in order to obtain short cycle times) and must not change their geometry in use thermal postprocessing inducing dimensional changes by postcrystallization may be necessary. In such cases parts should be stored in an oven with recirculated air at temperatures of 100 - 130 °C until dimensions don't change significantly any further. The time needed for this has to be determined experimentally.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.