Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® N2310 P AT - POM - BASF

Material Data Center offers the following functions for Ultraform® N2310 P AT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
含特性润滑剂的通用注塑等级。 低摩擦系数提供了极低的磨损和光滑的金属表面。


根据ISO 1043-1: POM的缩写名称
根据ISO 29988-POM-K,,M-GNRS2,3-2的名称
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 7.5 cm³/10min ISO 1133
温度 190 °C -
载荷 2.16 kg -
模塑收缩率, 平行 2.1 % ISO 294-4, 2577
模塑收缩率, 垂直 2.1 % ISO 294-4, 2577
喷射温度 110 °C -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2600 MPa ISO 527
屈服应力 61 MPa ISO 527
屈服伸长率 10 % ISO 527
名义断裂伸长率 31 % ISO 527
拉伸蠕变模量, 1h 1800 MPa ISO 899-1
拉伸蠕变模量, 1000h 1300 MPa ISO 899-1
无缺口简支梁冲击强度, +23°C 200 kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 180 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 6 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 5 kJ/m² ISO 179/1eA
悬臂梁缺口冲击强度, +23°C 6.5 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 6 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 - 温度 -30 °C -
球压硬度 135 MPa ISO 2039-1
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 166 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 90 °C ISO 75-1/-2
热变形温度, 0.45 MPa 157 °C ISO 75-1/-2
维卡软化温度, B 150 °C ISO 306
线性热膨胀系数, 平行 110 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.6 mm -
Yellow Card 现存 是的 - -
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
Yellow Card 现存 是的 - -
燃烧性-氧指数 15 % ISO 4589-1/-2
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 3.8 - IEC 62631-2-1
相对介电常数., 1MHz 3.8 - IEC 62631-2-1
介质损耗因子, 100Hz 10 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 50 E-4 IEC 62631-2-1
体积电阻率 1E12 Ohm*m IEC 62631-3-1
表面电阻率 1E12 Ohm IEC 62631-3-2
介电强度 40 kV/mm IEC 60243-1
相对漏电起痕指数 600 - IEC 60112
其它性能价值单位Test Standard
吸水性 0.9 % 类似ISO 62
吸湿性 0.2 % 类似ISO 62
密度 1410 kg/m³ ISO 1183
Bulk density 850 kg/m³ -
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 200 °C ISO 294
注塑, 模具温度 90 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
加工推荐(注塑)价值单位Test Standard
预干燥-温度 100 °C -
预干燥-时间 3 h -
加工湿度 ≤0.2 % -
注塑熔体温度 190 - 230 °C -
模具温度 60 - 120 °C -
函数
粘度-剪切速度 , Ultraform® N2310 P AT, POM, BASF
剪切应力-剪切速度 , Ultraform® N2310 P AT, POM, BASF
动态剪切模量-温度 , Ultraform® N2310 P AT, POM, BASF
应力-应变(等时的) 23°C, Ultraform® N2310 P AT, POM, BASF
应力-应变(等时的) 40°C, Ultraform® N2310 P AT, POM, BASF
应力-应变(等时的) 80°C, Ultraform® N2310 P AT, POM, BASF
比容-温度(pvT) , Ultraform® N2310 P AT, POM, BASF
典型数据
加工方法
注塑
供货形式
粒料
添加剂
润滑剂, 脱模助剂
特征
Tribologic Grade, 共聚物
应用
汽车
地区供应
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 190 - 230 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 60 - 120 °C
injection molding, Mold temperature, recommended: 90 °C
injection molding, Dwell time, thermoplastics: 10 min

Processing

Usual single-flighted three-section screws with an effective screw length of at least 15 D, better 20 - 23 D are suitable for the injection molding of Ultraform.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.


Postprocessing

If parts were produced at a comparatively low mold temperature (e.g. in order to obtain short cycle times) and must not change their geometry in use thermal postprocessing inducing dimensional changes by postcrystallization may be necessary. In such cases parts should be stored in an oven with recirculated air at temperatures of 100 - 130 °C until dimensions don't change significantly any further. The time needed for this has to be determined experimentally.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.