Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint PA11 ESD - PA11 - BASF

Material Data Center offers the following functions for Ultrasint PA11 ESD:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 20 / * cm³/10min ISO 1133
温度 220 / * °C -
载荷 2.16 / * kg -
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 204 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 111 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 186 / * °C ISO 75-1/-2
维卡软化温度, A 192 / * °C ISO 306
维卡软化温度, B 183 / * °C ISO 306
其它性能干 / 已调节单位Test Standard
密度 1070 / - kg/m³ ISO 1183
Bulk density 460 kg/m³ -
3D Data干 / 已调节单位Test Standard
Other Standards[S]
拉伸模量, flat 3150 / 2300 MPa ISO 527
拉伸模量, upright 2150 / 1550 MPa ISO 527
拉伸强度, flat 65 / 55 MPa ISO 527
拉伸强度, upright 55 / 47 MPa ISO 527
断裂伸长率, flat 20 / 22 % ISO 527
断裂伸长率, upright 23 / 31 % ISO 527
弯曲模量, flat 3050 / 2550 MPa ISO 178
弯曲模量, upright 2100 / 1650 MPa ISO 178
无缺口简支梁冲击强度, +23°C, flat 80 / 101 kJ/m² ISO 179/1eU
无缺口简支梁冲击强度, +23°C, upright 90 / 107 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C, flat 6.6 / 7.3 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, +23°C, upright 4.7 / 5.3 kJ/m² ISO 179/1eA
Izod冲击强度, +23°C, flat 67 / 81 kJ/m² ISO 180/1U
Izod冲击强度, +23°C, upright 58 / 83 kJ/m² ISO 180/1U
悬臂梁缺口冲击强度, +23°C, flat 7 / 7.9 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度, +23°C, upright 5 / 5.5 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
典型数据
加工方法
Additive Manufacturing, 镭射烧结
供货形式
粉料
耐化学试剂
通用耐化学性
Certifications
生物相容
应用
电子电气
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.