Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VECTRA® A700 - LCP-GF30 - Celanese

Material Data Center offers the following functions for VECTRA® A700:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vectra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Some conductivity. Suitable for electrostatic dissipation (ESD) applications. 30% glass reinforced. Chemical abbreviation according to ISO 1043-1 : LCP Inherently flame retardant UL-Listing V-0 at 0.42mm thickness per UL 94 flame testing. Relative-Temperature-Index (RTI) according to UL 746B: electrical 130°C, mechanical 130°C. UL = Underwriters Laboratories (USA)

Flammability at thickness hV-0-
加工/物理特性价值单位Test Standard
ISO数据
模塑收缩率, 平行 0.2 % ISO 294-4, 2577
模塑收缩率, 垂直 0.4 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 14000 MPa ISO 527
断裂应力 140 MPa ISO 527
断裂伸长率 1.5 % ISO 527
无缺口简支梁冲击强度, +23°C 15 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 7 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 280 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 232 °C ISO 75-1/-2
热变形温度, 0.45 MPa 250 °C ISO 75-1/-2
维卡软化温度, B 156 °C ISO 306
线性热膨胀系数, 平行 8 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 25 E-6/K ISO 11359-1/-2
厚度为h时的燃烧性 V-0 class IEC 60695-11-10
电性能价值单位Test Standard
ISO数据
体积电阻率 1000 Ohm*m IEC 62631-3-1
表面电阻率 1000000 Ohm IEC 62631-3-2
其它性能价值单位Test Standard
密度 1630 kg/m³ ISO 1183
典型数据
加工方法
注塑
供货形式
粒料
特殊性能
提高导电性, 防静电的, 阻燃的, 经光稳处理的/耐光的
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
其他信息
注塑成型
Vectra resins are well known for their excellent thermal and hydrolytic stability. In order to ensure these properties are optimum, the resin should be dried correctly prior to processing. Vectra A-grades should be dried at 150 C for a minimum of 4 hours in a desiccant dryer.
A three-zone screw evenly divided into feed, compression, and metering zones is preferred. A higher percentage of feed flights may be needed for smaller machines: 1/2 feed, 1/4 compression, 1/4 metering.

Vectra LCPs are shear thinning, their melt viscosity decreases quickly as shear rate increases. For parts that are difficult to fill, the molder can increase the injection velocity to improve melt flow.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com