Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® i2 G - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® i2 G:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Implantable grade polyether ether ketone resin for permanent implants

VESTAKEEP® i2 G is a natural colored, standard viscosity polyether ether ketone (PEEK) that is especially designed for long term implantable medical devices. This grade is often used for injection molding processing technologies due to its good flowability.

Proven Biocompatibility of VESTAKEEP® i-Grades
The extra high purity and extended quality measures make VESTAKEEP® i-Grade materials an excellent choice for permanent implants.

For VESTAKEEP® i2 G, biocompatibility has been tested following ISO 10993-1 recommendations for permanent tissue/bone contact and USP Class VI.

VESTAKEEP® i2 G complies ASTM F2026 “Standard Specification for Polyetheretherketone (PEEK) Polymers for Surgical Implant Applications”.

A summary of biocompatibility test results is available upon request.

Biocompatibility tests available for i2 G


Processing of VESTAKEEP® i-Grades
VESTAKEEP® i2 G can be processed by common melt processing techniques like injection molding and extrusion.

We recommend a melt temperature between 360°C and 380°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

Our technical experts would appreciate to give you support regarding the special requirements for the processing of VESTAKEEP® i2 G.

Delivery of VESTAKEEP® i-Grades
VESTAKEEP® i2 G is supplied as cylindrical pellets in 10 kg boxes with moisture-proof polyethylene liners.


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 68 cm³/10min ISO 1133
温度 380 °C -
载荷 5 kg -
模塑收缩率, 平行 1.1 % ISO 294-4, 2577
模塑收缩率, 垂直 1.1 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 3700 MPa ISO 527
屈服应力 98 MPa ISO 527
屈服伸长率 5 % ISO 527
名义断裂伸长率 20 % ISO 527
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
简支梁缺口冲击强度, -30°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 342 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 150 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 150 °C ISO 75-1/-2
热变形温度, 0.45 MPa 205 °C ISO 75-1/-2
维卡软化温度, B 310 °C ISO 306
线性热膨胀系数, 平行 60 E-6/K ISO 11359-1/-2
燃烧性-氧指数 38 % ISO 4589-1/-2
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 2.8 - IEC 62631-2-1
相对介电常数., 1MHz 2.8 - IEC 62631-2-1
介质损耗因子, 1MHz 50 E-4 IEC 62631-2-1
体积电阻率 >1E13 Ohm*m IEC 62631-3-1
相对漏电起痕指数 200 - IEC 60112
其它性能价值单位Test Standard
吸水性 0.4 % 类似ISO 62
吸湿性 0.12 % 类似ISO 62
密度 1300 kg/m³ ISO 1183
典型数据
加工方法
注塑, 其它挤出成型
供货形式
粒料, 自然色
Certifications
医用级, Biocompatibility ISO 10993, US药物六级认证
应用
药物
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.