Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® i2 UFP10 - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® i2 UFP10:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Ultra-fine polyether ether ketone (PEEK) powder for permanent implants
 
VESTAKEEP® i2 UFP10 is an unreinforced, medium-viscosity, natural colored polyether ether ketone (PEEK) ultra-fine powder.

VESTAKEEP® i2 UFP10 is especially designed for long term implantable medical devices.

The semi-crystalline polymer is designed for high biocompatibility and superior mechanical, thermal and chemical resistance.

Proven Biocompatibility of VESTAKEEP® i-Grades
The biocompatibility of VESTAKEEP® i2 UFP10 has been tested following ISO 10993 recommendations for permanent tissue/bone contact. The material complies USP Class VI.

VESTAKEEP® i2 UFP10 is compliant with ASTM F2026 “Standard Specification for Polyetheretherketone (PEEK) Polymers for Surgical Implant Applications”.

A summary of biocompatibility tests is available upon request.

Biocompatibility test reports available for i2 UFP10

 
In addition to the body contact period the suitability of the material depends on further criteria, for example the nature of the contact, the processing, or the surface. In any case the suitability has to be verified for the end product.

Processing of VESTAKEEP® i-Grades
For information about processing of VESTAKEEP® i2 UFP10, please follow the general recommendations in our brochure “High Performance in Powder Form - Polyether Ether Ketone Powders“.

Delivery of VESTAKEEP® i-Grades
VESTAKEEP® i2 UFP10 is supplied as a powder in 15 kg boxes or 5 kg buckets with moisture-proof polyethylene liners.

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 70 cm³/10min ISO 1133
温度 380 °C -
载荷 5 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 3700 MPa ISO 527
屈服应力 100 MPa ISO 527
屈服伸长率 5 % ISO 527
名义断裂伸长率 30 % ISO 527
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
简支梁缺口冲击强度, -30°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 340 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 155 °C ISO 75-1/-2
热变形温度, 0.45 MPa 205 °C ISO 75-1/-2
维卡软化温度, B 310 °C ISO 306
其它性能价值单位Test Standard
密度 1300 kg/m³ ISO 1183
典型数据
加工方法
表面涂层, 模压/烧结成型
供货形式
粉料, 自然色
特征
热稳定性
耐化学试剂
通用耐化学性
Certifications
医用级, Biocompatibility ISO 10993, US药物六级认证
应用
药物
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com