Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L1930 NC - PA12-GD30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L1930 NC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Milled glass fiber filled PA 12-Plastic resin for the injection molding

VESTAMID® L1930 NC is a heat stabilized, with 30% milled glass fiber-reinforced PA 12 compound suitable for injection molding of stiff, relatively warp free molded parts.

Due to the reinforcement moldings from this compound exhibit a high strength and rigidity. Because PA 12 absorbs only little water, the parts have a good dimensional stability and almost unaffected mechanical properties at changing ambient humidity.

Due to the reinforcement the shrinking of moldings is decreased compared with unreinforced compounds. Using specialty short glass fibers for the reinforcement of VESTAMID® L1930 NC the difference between longitudinal and transverse shrinkage relating to the flow direction of the melt is significantly lower than with common glass fiber-reinforced products. Therefore especially low-warpage precision parts can be molded.

As a semi-crystalline material VESTAMID® L1930 NC feature an outstanding chemical resistance, e.g., against fuels, oils and fats.

VESTAMID® L1930 NC is supplied as cylindrical pellets in moisture-proof packaging.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 24 / * cm³/10min ISO 1133
温度 240 / * °C -
载荷 5 / * kg -
模塑收缩率, 平行 0.7 / * % ISO 294-4, 2577
模塑收缩率, 垂直 0.6 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 3740 / - MPa ISO 527
屈服应力 63 / - MPa ISO 527
屈服伸长率 4.5 / - % ISO 527
名义断裂伸长率 12 / - % ISO 527
无缺口简支梁冲击强度, +23°C 89 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
简支梁冲击强度, -30°C 65 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
简支梁缺口冲击强度, +23°C 8 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
简支梁缺口冲击强度, -30°C 11 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 178 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 130 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 170 / * °C ISO 75-1/-2
维卡软化温度, B 170 / * °C ISO 306
线性热膨胀系数, 平行 50 / * E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 50 / * E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 1.5 / * mm -
Yellow Card 现存 是的 / * - -
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 0.8 / * mm -
Yellow Card 现存 是的 / * - -
电性能干 / 已调节单位Test Standard
ISO数据
相对介电常数., 100Hz 4.1 / - - IEC 62631-2-1
相对介电常数., 1MHz 3.4 / - - IEC 62631-2-1
介质损耗因子, 100Hz 310 / - E-4 IEC 62631-2-1
介质损耗因子, 1MHz 240 / - E-4 IEC 62631-2-1
体积电阻率 >1E13 / - Ohm*m IEC 62631-3-1
相对漏电起痕指数 600 / - - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 1.1 / * % 类似ISO 62
吸湿性 0.5 / * % 类似ISO 62
密度 1240 / - kg/m³ ISO 1183
函数
动态剪切模量-温度 , VESTAMID® L1930 NC (烘干), PA12-GD30, Evonik
典型数据
加工方法
注塑
供货形式
粒料, 自然色
添加剂
润滑剂
特殊性能
经热稳处理的/耐热的
特征
低翘曲
耐化学试剂
通用耐化学性, 耐油脂性, 耐油性
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.