Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9057 GN E60044 - PA12 FR(30+40) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9057 GN E60044:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Low viscosity, self-extinguishing polyamide 12 compound free of halogen

VESTAMID® LX9057 GN E60044 is a heat- stabilized compound with an efficient halogen-free flame retardant. Tested according to UL94, it complies with the flammability classification V-2.
 
The halogen-free formulation makes VESTAMID® LX9057 GN E60044 especially suitable for the electronic and cable industry.

VESTAMID® LX9057 GN E60044 can be used for injection molding as well as for wire extrusion coating. The semi-crystalline compounds based on PA12 only absorb small amounts of water.

Therefore manufactured parts exhibit excellent dimensional stability at changing ambient humidity, constant high toughness, low coefficient of friction and good chemical resistance.
  
Due to the presence of flame retardant the melt temperature should not exceed 240°C. We recommend melt temperatures of 200°C-220°C.
 
VESTAMID® LX9057 GN E60044 is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

The use of colorants may affect property values. 

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 1150 / - MPa ISO 527
屈服应力 36 / - MPa ISO 527
屈服伸长率 13 / - % ISO 527
名义断裂伸长率 >50 / - % ISO 527
无缺口简支梁冲击强度, +23°C 170 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
简支梁缺口冲击强度, +23°C 3 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 176 / * °C ISO 11357-1/-3
厚度为h时的燃烧性 V-2 / * class IEC 60695-11-10
测试用试样的厚度 0.8 / * mm -
其它性能干 / 已调节单位Test Standard
密度 1080 / - kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 220 °C ISO 294
注塑, 模具温度 80 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
典型数据
加工方法
注塑, 表面涂层
供货形式
粒料
特殊性能
阻燃的, 无卤, 经热稳处理的/耐热的
特征
Tribologic Grade
耐化学试剂
通用耐化学性
应用
电子电气
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.