Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® X7393 NC - PA12-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® X7393 NC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

High viscosity, plasticized, impact modified, heat- and light stabilized polyamide 12 compound

VESTAMID® X7393  is a high viscosity, plasticized, impact modified, heat- and light stabilized polyamide 12 compound for flexible tubing and hoses for the automobile industry according to DIN 73 378 and DIN 74 324,Type PA 12-PHLY.

Parts made of VESTAMID® X7393 are characterized by optimized cold temperature impact resistance for the extrusion of semi-rigid tubing with increased burst pressure resistance as well as exceptional low coefficient of friction and good chemical resistance. Properties of compounds based on Polyamide 12 vary little with changing humidity due to their low moisture absorption.

VESTAMID® X7393 is supplied as pellets, ready for use, in moisture-proof bags.

The use of colorants may affect property values. 

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

加工/物理特性干 / 已调节单位Test Standard
ISO数据
熔体体积流动速度, MVR 8.5 / * cm³/10min ISO 1133
温度 230 / * °C -
载荷 5 / * kg -
模塑收缩率, 平行 0.8 / * % ISO 294-4, 2577
模塑收缩率, 垂直 1.4 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 520 / 470 MPa ISO 527
屈服应力 29 / 27 MPa ISO 527
屈服伸长率 28 / 28 % ISO 527
名义断裂伸长率 >50 / >50 % ISO 527
无缺口简支梁冲击强度, +23°C N / N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N / N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 108 / 130 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 7 / 8 kJ/m² ISO 179/1eA
Type of failure C / C - -
肖氏硬度D 67 / * - ISO 7619-1
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 177 / * °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 15 / * °C ISO 11357-1/-2
热变形温度, 1.80 MPa 45 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 110 / * °C ISO 75-1/-2
维卡软化温度, B 125 / * °C ISO 306
其它性能干 / 已调节单位Test Standard
吸水性 1.2 / * % 类似ISO 62
吸湿性 0.7 / * % 类似ISO 62
密度 1020 / - kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 熔体温度 220 °C ISO 294
注塑, 模具温度 60 °C ISO 294
注塑, 注射速度 200 mm/s ISO 294
典型数据
加工方法
管材挤出
供货形式
粒料, 自然色
添加剂
增塑剂
特殊性能
高冲击韧性的/经抗冲改性的, 经光稳处理的/耐光的, 经热稳处理的/耐热的
特征
Tribologic Grade
耐化学试剂
通用耐化学性
应用
汽车
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.