Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTODUR® 2000 - PBT - Evonik Operations GmbH

Material Data Center offers the following functions for VESTODUR® 2000:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Vestodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Medium-viscosity, Polybutylen terephthalat resin

VESTODUR® 2000 is a medium-viscosity, unreinforced, semi-crystalline Polybutylen terephthalat resin for injection molding and extrusion.

The resin features superior thermal and mechanical resistance.

VESTODUR® 2000 is supplied as granules in polyethylene containers.
 
Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT WWW.VESTODUR.COM
函数
粘度-剪切速度 , VESTODUR® 2000, PBT, Evonik
剪切应力-剪切速度 , VESTODUR® 2000, PBT, Evonik
应力-应变.  , VESTODUR® 2000, PBT, Evonik
正割模量-应变.  , VESTODUR® 2000, PBT, Evonik
应力-应变(等时的) 23°C, VESTODUR® 2000, PBT, Evonik
蠕变模量-时间. 23°C, VESTODUR® 2000, PBT, Evonik
蠕变曲线 23°C, VESTODUR® 2000, PBT, Evonik
比容-温度(pvT) , VESTODUR® 2000, PBT, Evonik
单位质量比焓-温度(DSC) , VESTODUR® 2000, PBT, Evonik
拉伸模量-温度 , VESTODUR® 2000, PBT, Evonik
典型数据
加工方法
注塑, 薄膜挤出成型, 片材挤出成型, 其它挤出成型, 表面涂层
供货形式
粒料
特殊性能
经光稳处理的/耐光的
特征
热稳定性
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.