Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTORAN® X7342 - PPE-GF20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTORAN® X7342:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestoran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Modified polyphenylene ether (PPE), high heat resistant, 20 % glass fiber-reinforced

VESTORAN® X7342 is the registered trademark of the Evonik Degussa GmbH for molding compounds containing poly-2,6-dimethyl-1,4-phenylene ether as polymeric constituent (poly-phenylene ether, PPE, also referred to as PPO).

As a material of amorphous structure, VESTORAN® X7342 shows very small mold shrinkage. Therefore molded parts have a very low tendency to warp.

Moldings of VESTORAN® X7342 are dimen­sionally stable and hydrolysis resistant even in hot water, but are more sensitive to organic solvents than semi-crystalline plastics. VESTORAN® X7342 is resistant to aqueous alkalines and acides, certain alcohols, and glycol solutions.

Due to the glass fiber-reinforcement the compound combines outstanding heat deflection temperature under load with high strength and rigidity. The even smaller shrinkage compared to non-reinforced VESTORAN® depends on the orientation of the glass fibers in the molded part.
 
VESTORAN® X7342 is supplied as cylindrical granules in polyethylene packaging.
 
Processing advice is given in a separate product information.

Pigmentation may affect values.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 40 cm³/10min ISO 1133
温度 300 °C -
载荷 21.6 kg -
模塑收缩率, 平行 0.2 % ISO 294-4, 2577
模塑收缩率, 垂直 0.4 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 6100 MPa ISO 527
断裂应力 108 MPa ISO 527
断裂伸长率 3.5 % ISO 527
无缺口简支梁冲击强度, +23°C 49 kJ/m² ISO 179/1eU
Type of failure C - -
简支梁缺口冲击强度, +23°C 13 kJ/m² ISO 179/1eA
Type of failure C - -
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 165 °C ISO 75-1/-2
热变形温度, 0.45 MPa 170 °C ISO 75-1/-2
维卡软化温度, B 170 °C ISO 306
线性热膨胀系数, 平行 40 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 30 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 1.6 mm -
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 0.8 mm -
Yellow Card 现存 是的 - -
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 3 - IEC 62631-2-1
相对介电常数., 1MHz 3.5 - IEC 62631-2-1
介质损耗因子, 100Hz 80 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 10 E-4 IEC 62631-2-1
体积电阻率 1E11 Ohm*m IEC 62631-3-1
相对漏电起痕指数 175 - IEC 60112
其它性能价值单位Test Standard
密度 1190 kg/m³ ISO 1183
典型数据
加工方法
注塑
供货形式
粒料
特殊性能
经热稳处理的/耐热的
特征
无定形, 低翘曲
耐化学试剂
耐酸性, 耐碱性, 水解稳定
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.