Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® 85XFS - PA66/6 - Ascend

Material Data Center offers the following functions for Vydyne® 85XFS:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Vydyne 85XFS is a general purpose PA66/6 copolymer resin designed for extrusion-compounding applications. It is available in natural only. This copolymer resin provides a lower melting point and can be used for compounding thermally sensitive additives or fillers. It offers a well balanced combination of engineering properties characterized by high strength, rigidity, good toughness, high melt point, good surface lubricity, and abrasion resistance. Vydyne 85XFS exhibits chemical resistance to many chemicals, machine and motor oils, solvents, and gasoline.
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 245 / * °C ISO 11357-1/-3
其它性能干 / 已调节单位Test Standard
密度 1140 / - kg/m³ ISO 1183
典型数据
加工方法
其它挤出成型
供货形式
粒料, 自然色
特征
共聚物
耐化学试剂
通用耐化学性, 耐溶剂性, 耐油性
应用
通用
地区供应
北美, 欧洲, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.