Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of XAREC® WA 552 CJ772004 - (PS-SY)-GF30 - Idemitsu Chemicals
Material Data Center offers the following functions for XAREC® WA 552 CJ772004:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Xarec datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
加工/物理特性 | 价值 | 单位 | Test Standard |
Other Standards[S] |
模塑收缩率, 平行 |
0.2 |
% |
Producer Method |
模塑收缩率, 垂直 |
0.5 |
% |
Producer Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
机械性能 | 价值 | 单位 | Test Standard |
ISO数据 |
拉伸模量 |
9100 |
MPa |
ISO 527 |
断裂应力 |
120 |
MPa |
ISO 527 |
断裂伸长率 |
2.3 |
% |
ISO 527 |
弯曲模量, 23°C |
8900 |
MPa |
ISO 178 |
弯曲强度 |
185 |
MPa |
ISO 178 |
简支梁冲击强度, +23°C |
50 |
kJ/m² |
ISO 179/1eU |
简支梁缺口冲击强度, +23°C |
14 |
kJ/m² |
ISO 179/1eA |
Izod冲击强度, +23°C |
41 |
kJ/m² |
ISO 180/1U |
悬臂梁缺口冲击强度, +23°C |
13 |
kJ/m² |
ISO 180/1A |
热性能 | 价值 | 单位 | Test Standard |
ISO数据 |
热变形温度, 1.80 MPa |
235 |
°C |
ISO 75-1/-2 |
热变形温度, 0.45 MPa |
265 |
°C |
ISO 75-1/-2 |
线性热膨胀系数, 平行 |
23 |
E-6/K |
ISO 11359-1/-2 |
线性热膨胀系数, 垂直 |
59 |
E-6/K |
ISO 11359-1/-2 |
1.5mm名义厚度时的燃烧性 |
HB |
class |
IEC 60695-11-10 |
测试用试样的厚度 |
1.5 |
mm |
- |
Yellow Card 现存 |
是的 |
- |
- |
电性能 | 价值 | 单位 | Test Standard |
ISO数据 |
相对漏电起痕指数 |
500 |
- |
IEC 60112 |
ASTM数据 |
电介质强度, 短时 |
28 |
kV/mm |
ASTM D 149 |
耐电弧性 |
150 |
s |
ASTM D 495 |
Other Standards[S] |
相对介电常数, 1MHz |
3.1 |
- |
IEC 60250 |
介质损耗因子, 1MHz |
10 |
E-4 |
IEC 60250 |
体积电阻率 |
1E14 |
Ohm*m |
IEC 60093 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
其它性能 | 价值 | 单位 | Test Standard |
密度 |
1250 |
kg/m³ |
ISO 1183 |
加工推荐(注塑) | 价值 | 单位 | Test Standard |
预干燥-温度 |
120 |
°C |
- |
预干燥-时间 |
3 - 5 |
h |
- |
注塑熔体温度 |
280 - 310 |
°C |
- |
模具温度 |
130 - 155 |
°C |
- |
典型数据
加工方法
注塑
供货形式
粒料, 黑色
特殊性能
高冲击韧性的/经抗冲改性的
Certifications
可食品接触的, 可水接触的, NSF认证 61
应用
汽车, 电子电气
地区供应
北美, 欧洲, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.