Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ZYPEEK® 770CA30 - PEEK-CF - Jilin Joinature Polymer Co.,Ltd.

Material Data Center offers the following functions for ZYPEEK® 770CA30:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Zypeek datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 2.3 g/10min ISO 1133
温度 380 °C -
负载 5 kg -
模塑收缩率, 平行 0.1 % ISO 294-4, 2577
模塑收缩率, 垂直 0.5 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
断裂应力 260 MPa ISO 527
断裂伸长率 1.7 % ISO 527
弯曲模量, 23°C 23000 MPa ISO 178
简支梁冲击强度, +23°C 45 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 7 kJ/m² ISO 179/1eA
Izod冲击强度, +23°C 45 kJ/m² ISO 180/1U
悬臂梁缺口冲击强度, +23°C 9 kJ/m² ISO 180/1A
肖氏硬度D 88 - ISO 7619-1
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 343 °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 143 °C ISO 11357-1/-2
热变形温度, 1.80 MPa 336 °C ISO 75-1/-2
线性热膨胀系数, 平行 5 E-6/K ISO 11359-1/-2
电性能价值单位Test Standard
ISO数据
体积电阻率 1000 Ohm*m IEC 62631-3-1
其它性能价值单位Test Standard
吸水性 0.3 % 类似ISO 62
密度 1400 kg/m³ ISO 1183
典型数据
加工方法
注塑, 其它挤出成型
特殊性能
阻燃的, 经热稳处理的/耐热的
特征
防蠕变, Tribologic Grade
地区供应
亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.