Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Adsyl 7623 XCP - PP - LyondellBasell Industries

Material Data Center offers the following functions for Adsyl 7623 XCP:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Adsyl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 5.5 g/10min ISO 1133
温度 230 °C -
负载 2.16 kg -
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 132 °C ISO 11357-1/-3
热变形温度, 0.45 MPa 62 °C ISO 75-1/-2
维卡软化温度, A 107 °C ISO 306
光学特性价值单位Test Standard
ASTM数据
光泽度 87 - ASTM D 2457
雾度 1.2 % ASTM D 1003
其它性能价值单位Test Standard
密度 900 kg/m³ ISO 1183
机械性能(薄膜)价值单位Test Standard
ISO数据
拉伸模量, 平行 280 MPa ISO 527-3
拉伸模量, 垂直 280 MPa ISO 527-3
屈服应力, 平行 14 MPa ISO 527-3
屈服应力, normal 14 MPa ISO 527-3
屈服应变., 平行 17 % ISO 527-3
屈服应变., 垂直 15 % ISO 527-3
断裂应力, 平行 45 MPa ISO 527-3
断裂应力, 垂直 35 MPa ISO 527-3
最大应变, 平行 900 % ISO 527-3
最大应变, normal 800 % ISO 527-3
挤出形式 陆陇 - -
试样厚度 0.05 mm -
典型数据
加工方法
薄膜挤出成型
添加剂
防结块剂
特征
可热封的
Certifications
可食品接触的
应用
包装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.