Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Bakelite® PF 2774 - PF-(GF+X) - Bakelite Synthetics

Material Data Center offers the following functions for Bakelite® PF 2774:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Bakelite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

产品说明:

酚醛树脂成型材料,无机物充填,玻璃纤维补强,提高尺寸安定性,中等切口耐冲击强度,中等耐热性,改善电气特性,通过UL认证的成型材料1.5 mm / V-0(全色系)

应用:

接触器,帮浦零件,绝缘法兰,汽车引擎组件,刹车动力电瓶,转向端板及灯座。

加工/物理特性价值单位Test Standard
ISO数据
模塑收缩率, 平行 0.4 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 10000 MPa ISO 527
无缺口简支梁冲击强度, +23°C 8.5 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 2.4 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
热变形温度, 8.00 MPa 150 °C ISO 75-1/-2
1.5mm名义厚度时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
Yellow Card 现存 是的 - -
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 7.5 - IEC 62631-2-1
介质损耗因子, 100Hz 0.15 E-4 IEC 62631-2-1
体积电阻率 1E10 Ohm*m IEC 62631-3-1
表面电阻率 1E11 Ohm IEC 62631-3-2
介电强度 26.5 kV/mm IEC 60243-1
相对漏电起痕指数 175 - IEC 60112
其它性能价值单位Test Standard
密度 1700 kg/m³ ISO 1183
试样制备条件价值单位Test Standard
ISO数据
注塑, 塑化熔体温度 115 °C ISO 10724
注塑, 注射速度 170 mm/s ISO 10724
注塑, 保压压力 100 MPa ISO 10724
注塑, 固化时间 25 min ISO 10724
压缩, 模具温度 160 °C ISO 295
压缩, 固化时间 1 min ISO 295
函数
动态剪切模量-温度 , Bakelite® PF 2774, PF-(GF+X), Bakelite Synthetics
应力-应变.  , Bakelite® PF 2774, PF-(GF+X), Bakelite Synthetics
正割模量-应变.  , Bakelite® PF 2774, PF-(GF+X), Bakelite Synthetics
典型数据
加工方法
注塑, 模压/烧结成型
地区供应
其他信息
注塑成型
VERARBEITUNG 
Temperature of material: 80 - 100 °C
Mould temperature: 160 - 190 °C
Curing time: 10-20 sec
 
Further Information:
Barrel temperature
  - Feed zone: 60-75 °C
  - Nozzle zone: 80-100 °C
Cavity moulding pressure: >15 MPa
Back pressure: 0.5-2 MPa
Holding pressure: 60% of injection pressure
模压成型
PROCESSING
Mould temperature:160-190°C
Curing time:20-40sec
Cavity moulding pressure: >15MPa
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.