Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Clyrell EC2218 - PP - PolyMirae

Material Data Center offers the following functions for Clyrell EC2218:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Clyrell datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 7 g/10min ISO 1133
温度 230 °C -
ASTM数据
熔融指数, MFI 7 g/10min ASTM D 1238
温度 230 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
屈服应力 24 MPa ISO 527
屈服伸长率 12 % ISO 527
弯曲模量, 23°C 1000 MPa ISO 178
悬臂梁缺口冲击强度, +23°C 14 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 3 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度 - 温度 -20 °C -
ASTM数据
屈服应力 23.5 MPa ASTM D 638
弯曲模量 981 MPa ASTM D 790
悬臂梁缺口冲击强度, 1/8 in 132 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 27.9 J/m ASTM D 256
温度 -20 °C -
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 163 °C ISO 11357-1/-3
热变形温度, 0.45 MPa 87 °C ISO 75-1/-2
ASTM数据
DTUL @ 66 psi 87 °C ASTM D 648
其它性能价值单位Test Standard
密度 900 kg/m³ ISO 1183
典型数据
加工方法
薄膜挤出成型, 热成型
特殊性能
经热稳处理的/耐热的, 透明.
特征
防潮性/低应力发白, 好粘附性能, 可热封的, 低凝胶, 共聚物
应用
包装
地区供应
亚太, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.