Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of COOLPOLY® E5101 - PPS - Celanese

Material Data Center offers the following functions for COOLPOLY® E5101:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other CoolPoly datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
CoolPoly E series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows design freedom in applications previously restricted to metals. The E series is electrically conductive and provides inherent EMI/RFI shielding characteristics.

Flammability at thickness h (1 mm)V-0-
机械性能价值单位Test Standard
ISO数据
拉伸模量 11600 MPa ISO 527
断裂应力 44 MPa ISO 527
断裂伸长率 0.43 % ISO 527
无缺口简支梁冲击强度, +23°C 3.5 kJ/m² ISO 179/1eU
热性能价值单位Test Standard
ISO数据
熔融温度, 10°C/min 280 °C ISO 11357-1/-3
热变形温度, 1.80 MPa 248 °C ISO 75-1/-2
热变形温度, 0.45 MPa 279 °C ISO 75-1/-2
厚度为h时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 1.0 mm -
电性能价值单位Test Standard
ISO数据
体积电阻率 0.0017 Ohm*m IEC 62631-3-1
其它性能价值单位Test Standard
吸水性 0.05 % 类似ISO 62
密度 1710 kg/m³ ISO 1183
函数
应力-应变.  , COOLPOLY® E5101, PPS, Celanese
正割模量-应变.  , COOLPOLY® E5101, PPS, Celanese
典型数据
加工方法
注塑
特殊性能
提高导电性, 导热性
特征
EMI衰减/防护
地区供应
北美, 欧洲, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.