Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DOWLEX™ GM 8090 - (PE-LLD) - The Dow Chemical Company

Material Data Center offers the following functions for DOWLEX™ GM 8090:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Dowlex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
熔融指数, MFI 1 g/10min ASTM D 1238
温度 190 °C -
负载 2.16 kg -
热性能价值单位Test Standard
ASTM数据
熔点 111 °C ASTM D 3418
维卡温度 108 °C ASTM D 1525
光学特性价值单位Test Standard
ASTM数据
光泽度 47 - ASTM D 2457
雾度 14 % ASTM D 1003
其它性能价值单位Test Standard
密度 916 kg/m³ ASTM D 792
机械性能(薄膜)价值单位Test Standard
ASTM Data
屈服应力, 平行 6 MPa ASTM D 882
屈服应力, 垂直 7.3 MPa ASTM D 882
断裂拉伸强度, 平行 27 MPa ASTM D 882
断裂拉伸强度, 垂直 28 MPa ASTM D 882
断裂伸长率, 平行 500 % ASTM D 882
断裂伸长率, 垂直 550 % ASTM D 882
试样厚度 0.05 mm -
加工推荐(挤出)价值单位Test Standard
Type of extrusion blown - -
注塑熔体温度 190 - 240 °C -
典型数据
加工方法
吹塑挤出成型, 薄膜挤出成型
特殊性能
透明.
特征
可热封的, 低凝胶
Certifications
可食品接触的, 10/2011认证, FDA 21 CFR认证, Food contact notification (FCN)
应用
包装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.