Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DURACON® HP270X - POM - Polyplastics

Material Data Center offers the following functions for DURACON® HP270X:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Duracon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 22 cm³/10min ISO 1133
温度 190 °C -
载荷 2.16 kg -
熔融指数, MFI 26 g/10min ISO 1133
温度 190 °C -
负载 2.16 kg -
模塑收缩率, 平行 2.0 % ISO 294-4, 2577
模塑收缩率, 垂直 2.3 % ISO 294-4, 2577
机械性能价值单位Test Standard
ISO数据
拉伸模量 3050 MPa ISO 527
拉伸强度 69 MPa ISO 527
名义断裂伸长率 25 % ISO 527
弯曲模量, 23°C 2800 MPa ISO 178
弯曲强度 98 MPa ISO 178
简支梁缺口冲击强度, +23°C 6 kJ/m² ISO 179/1eA
洛克硬度 M 90 - ISO 2039-2
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 100 °C ISO 75-1/-2
线性热膨胀系数, 平行 110 E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 110 E-6/K ISO 11359-1/-2
厚度为h时的燃烧性 HB class IEC 60695-11-10
Yellow Card 现存 是的 - -
电性能价值单位Test Standard
ISO数据
体积电阻率 1E12 Ohm*m IEC 62631-3-1
表面电阻率 1E16 Ohm IEC 62631-3-2
介电强度 19 kV/mm IEC 60243-1
其它性能价值单位Test Standard
密度 1410 kg/m³ ISO 1183
典型数据
特殊性能
经热稳处理的/耐热的
耐化学试剂
通用耐化学性, 耐油脂性
地区供应
亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com