Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ A150 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ A150:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastar™ A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethanol. Eastar™ A150 is

intended primarily for extrusion into film and sheeting for packaging applications. It has excellent hydrolytic stability and good heat stability. Eastar™ A150 copolyester is lawful for use in food contact applications under food additive regulations published at 21 CFR 177.1240 by the Federal Food and Drug Administration. Therefore, it is lawful for use as a packaging material for meat or poultry foods prepared under federal inspection of the U.S. Department of Agriculture regulations at 9 CFR 318.7 and 381.147.




热性能价值单位Test Standard
ASTM数据
熔点 261 °C ASTM D 3418
玻璃化转变温度 91 °C ASTM E 1356
光学特性价值单位Test Standard
ASTM数据
光泽度 108 - ASTM D 2457
雾度 0.5 % ASTM D 1003
光透射率 93 % ASTM D 1003
其它性能价值单位Test Standard
密度 1200 kg/m³ ASTM D 792
Bulk Density 670 kg/m³ -
机械性能(薄膜)价值单位Test Standard
ASTM Data
拉伸模量, 平行 1600 MPa ASTM D 882
拉伸模量, 垂直 1600 MPa ASTM D 882
屈服应力, 平行 43 MPa ASTM D 882
屈服应力, 垂直 43 MPa ASTM D 882
断裂拉伸强度, 平行 56 MPa ASTM D 882
断裂拉伸强度, 垂直 56 MPa ASTM D 882
屈服伸长率, 平行 5 % ASTM D 882
屈服伸长率, 垂直 5 % ASTM D 882
断裂伸长率, 平行 250 % ASTM D 882
断裂伸长率, 垂直 250 % ASTM D 882
试样厚度 0.28 mm -
典型数据
加工方法
薄膜挤出成型, 片材挤出成型
特殊性能
经热稳处理的/耐热的, 透明.
特征
共聚物
耐化学试剂
水解稳定
Certifications
可食品接触的, FDA 21 CFR认证
应用
包装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.