Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EN076 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EN076:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Eastar™ EN076 copolyester is a clear copolyester used in a variety of packaging and consumer product applications, including food and beverage packaging, general purpose packaging, flexible film packaging, and consumer products. It is fully compatible with the resin identification code 1 (RIC1) recycle stream. Eastar EN076

enables fast-moving consumer-goods brand owners to achieve recyclable products and packaging and replace materials of concern without sacrificing aesthetics.


Eastar EN076 meets the definition of resin identification code PREPROCESSING (RIC1) as defined by ASTM D7611. Other endproduct attributes, including but not limited to size, color, auxiliary components, and availability of collection, may also impact recyclability.


Eastar EN076 copolyester may be used in various food contact applications under the U.S. Food & Drug Administration (FDA) regulations.




加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.0035 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
屈服应力 56 MPa ASTM D 638
断裂拉伸强度 26 MPa ASTM D 638
屈服伸长率 4 % ASTM D 638
断裂伸长率 75 % ASTM D 638
弯曲模量 2350 MPa ASTM D 790
洛克硬度 111 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in 67 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 33 J/m ASTM D 256
温度 -40 °C -
Izod冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
DTUL @ 66 psi 69 °C ASTM D 648
DTUL @ 264 psi 62 °C ASTM D 648
光学特性价值单位Test Standard
ASTM数据
雾度 0.8 % ASTM D 1003
光透射率 89 % ASTM D 1003
其它性能价值单位Test Standard
密度 1320 kg/m³ ASTM D 792
加工推荐(挤出)价值单位Test Standard
预干燥-温度 150 °C -
预干燥-时间 4 - 6 h -
注塑熔体温度 277 - 293 °C -
模具温度 16 - 32 °C -
典型数据
加工方法
注塑, 薄膜挤出成型, 其它挤出成型, 热成型
特征
共聚物
Certifications
可食品接触的, FDA 21 CFR认证
应用
包装
地区供应
北美, 欧洲, 亚太, 中南美洲, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.