Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ECONAMID FL 6G30 - PA6-GF30 - DOMO Engineering Plastics

Material Data Center offers the following functions for ECONAMID FL 6G30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Econamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性干 / 已调节单位Test Standard
ISO数据
模塑收缩率, 平行 0.3 / * % ISO 294-4, 2577
模塑收缩率, 垂直 0.8 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 9000 / 5700 MPa ISO 527
断裂应力 140 / 90 MPa ISO 527
断裂伸长率 3 / 6 % ISO 527
弯曲模量, 23°C 7500 / 4400 MPa ISO 178
简支梁冲击强度, +23°C 40 / 55 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 6 / 10 kJ/m² ISO 179/1eA
Izod冲击强度, +23°C 35 / 50 kJ/m² ISO 180/1U
悬臂梁缺口冲击强度, +23°C 5.5 / 10 kJ/m² ISO 180/1A
洛克硬度 R 122 - ISO 2039-2
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 221 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 200 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 215 / * °C ISO 75-1/-2
维卡软化温度, B 210 / * °C ISO 306
厚度为h时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 0.8 / * mm -
电性能干 / 已调节单位Test Standard
ISO数据
体积电阻率 1E13 / - Ohm*m IEC 62631-3-1
表面电阻率 * / 1E13 Ohm IEC 62631-3-2
其它性能干 / 已调节单位Test Standard
密度 1360 / - kg/m³ ISO 1183
模塑测量的特殊性能干 / 已调节单位Test Standard
ISO数据
粘数. 135 / * cm³/g ISO 307, 1157, 1628
加工推荐(注塑)价值单位Test Standard
预干燥-温度 75 - 85 °C -
预干燥-时间 2 - 4 h -
注塑熔体温度 240 - 270 °C -
模具温度 90 - 100 °C -
典型数据
加工方法
注塑
地区供应
北美, 欧洲, 亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.