Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ECOZEN® YH 100 - TPC - SK Chemicals

Material Data Center offers the following functions for ECOZEN® YH 100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ecozen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
加工/物理特性价值单位Test Standard
ASTM数据
模压收缩率, 平行 0.0035 mm/mm ASTM D 955
机械性能价值单位Test Standard
ASTM数据
屈服应力 51 MPa ASTM D 638
断裂拉伸强度 42 MPa ASTM D 638
屈服伸长率 5.7 % ASTM D 638
断裂伸长率 150 % ASTM D 638
弯曲模量 2130 MPa ASTM D 790
弯曲强度 86 MPa ASTM D 790
洛克硬度 R 115 - ASTM D 785
悬臂梁缺口冲击强度, 1/8 in N J/m ASTM D 256
热性能价值单位Test Standard
ASTM数据
DTUL @ 66 psi 85 °C ASTM D 648
光学特性价值单位Test Standard
ASTM数据
雾度 1 % ASTM D 1003
光透射率 89 % ASTM D 1003
其它性能价值单位Test Standard
密度 1250 kg/m³ ASTM D 792
典型数据
特殊性能
高冲击韧性的/经抗冲改性的, 透明.
特征
共聚物
耐化学试剂
通用耐化学性, 耐污染性
Certifications
生物相容
应用
包装
地区供应
北美, 欧洲, 亚太, 中南美洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.